# US 10,954,368 B2 · Block copolymer-toughened isotactic polypropylene

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,368 B2
- Document ID: US10954368B2
- Status: Granted
- Kind: B2
- Application number: 16/378,970
- Filed: 2019-04-09
- Published: 2019-10-10
- Granted: 2021-03-23
- Earliest claimed: 2018-04-10
- Assignees: Regents of the University of Minnesota
- Applicants: Regents of the University of Minnesota
- Inventors: Jun Xu; Frank S. Bates
- Web page: https://patentgrep.com/patent/US10954368B2

## CPC

- C08L 23/12: Polypropene
- C08L 23/08: Copolymers of ethene (C08L23/16 takes precedence)
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2207/02: Heterophasic composition
- C08L 2207/10: Peculiar tacticity
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A blend that includes (a) a continuous phase comprising isotactic polypropylene and (b) a dispersed phase comprising a poly-(ethylene-alt-propylene)-b-poly(ethylene-ran-ethyl ethylene) diblock copolymer. The amount of diblock copolymer is less than 20 wt % based on the total weight of the blend.

## Claims

### Claim 1

A blend comprising (a) a continuous phase comprising isotactic polypropylene and (b) a dispersed phase comprising a poly-(ethylene-alt-propylene)-b-poly(ethylene-ran-ethylethylene) diblock copolymer, wherein the amount of diblock copolymer is less than 20 wt % based on the total weight of the blend.

### Claim 2 (depends on 1)

The blend of claim 1 wherein the amount of diblock copolymer is no greater than 10 wt % based on the total weight of the blend.

### Claim 3 (depends on 1)

The blend of claim 1 wherein the amount of diblock copolymer is no greater than 5 wt % based on the total weight of the blend.

### Claim 4 (depends on 1)

The blend of claim 1 wherein the amount of diblock copolymer is no greater than 2.5 wt % based on the total weight of the blend.

### Claim 5 (depends on 1)

The blend of claim 1 wherein the amount of diblock copolymer is between 1 and 5 wt % based on the total weight of the blend.

### Claim 6 (depends on 1)

The blend of claim 1 wherein the diblock copolymer is in the form of micelles having an average diameter no greater than 150 nm.

### Claim 7 (depends on 1)

The blend of claim 1 wherein the diblock copolymer is in the form of micelles having an average diameter no greater than 100 nm.

### Claim 8 (depends on 1)

The blend of claim 1 wherein the blend has an Izod impact strength that is at least 5 times greater than the Izod impact strength of an identical blend that lacks the block copolymer.

### Claim 9 (depends on 1)

The blend of claim 1 wherein the blend has an Izod impact strength that is at least 10 times greater than the Izod impact strength of an identical blend that lacks the block copolymer.

### Claim 10 (depends on 1)

The blend of claim 1, wherein the blend has a tensile strain at break that is at least 20 times greater than the tensile strain at break of an identical blend that lacks the block copolymer.

### Claim 11

A blend comprising (a) a continuous phase comprising isotactic polypropylene and (b) a dispersed phase comprising a poly-(ethylene-alt-propylene)-b-poly(ethylene-ran-ethyl ethylene) diblock copolymer in the form of micelles having an average diameter no greater than 150 nm, wherein (i) the amount of diblock copolymer is less than 10 wt % based on the total weight of the blend, (ii) the blend has an Izod impact strength that is at least 5 times greater than the Izod impact strength of an identical blend that lacks the block copolymer, and (iii) the blend has a tensile strain at break that is at least 20 times greater than the tensile strain at break of an identical blend that lacks the block copolymer.