# US 10,954,355 B2 · Reusable capture complex

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,355 B2
- Document ID: US10954355B2
- Status: Granted
- Kind: B2
- Application number: 16/419,248
- Filed: 2019-05-22
- Published: 2019-11-07
- Granted: 2021-03-23
- Earliest claimed: 2014-12-23
- Assignees: Ioniqa Techonolgies B.V.
- Applicants: Ioniqa Technologies B.V.
- Inventors: Susanne Van Berkum; Vincent Philippi; Marcel Vilaplana Artigas; Rick De Groot; Tonnis Hooghoudt
- Web page: https://patentgrep.com/patent/US10954355B2

## CPC

- C08J 11/28: by treatment with organic compounds containing nitrogen, sulfur or phosphorus
- C08J 11/04: of polymers
- C08J 11/16: by treatment with inorganic material (C08J11/14 takes precedence)
- C08J 11/24: containing hydroxyl groups
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention is in the field of an improved reusable capture complex and a method of releasable capturing an additive present in a polymer material. The capture complex comprises a catalyst entity, a magnetic nanoparticle, and a bridging moiety solely between the catalyst entity and the magnetic nanoparticle The present use and method provide a high reduction of free additive of a polymer material.

## Claims

### Claim 1

Method of degrading a mixture of waste polymers comprising polymer material and additives, which additives are released from the waste polymer the additive upon degradation of the polymer material, which method comprises the steps of:
providing an improved reusable capture complex;
providing the mixture of waste polymers in solid form in a solvent wherein the polymer material is one or more of a polyester, a polyamide, a polyamine and a polyether, and wherein the solvent is a mono- or di-alcohol;
degrading the polymer material by glycolysis, wherein the solvent functions as a reactant, and wherein the capture complex catalyses degradation of the polymer material, wherein the additive is released from the polymer and wherein a mixture is obtained;
cooling down the obtained mixture to 50-85° C.;
using the capture complex to capture the additive;
performing a separation to separate the capture complex with the captured additive from the mixture;
cooling the mixture further in order to precipitate a monomer and dimer from the polymer material,
wherein the improved capture complex is not dispersible in water and comprising a catalyst entity, a magnetic nanoparticle, and a bridging moiety solely between the catalyst entity and the magnetic nanoparticle, wherein the catalyst entity and bridging moiety are attached, and wherein the bridging moiety and nanoparticle are attached,
wherein the catalyst entity comprises an aromatic heterocycle moiety provided with at least one nitrogen atom and carrying a positive charge, and a negatively charged moiety, wherein the negative charge is on a metal salt complex moiety having a two- or three-plus charged metal ion or a negatively charged counter-ion,
wherein the nanoparticles have an average diameter of 2 nm-500 nm, and
wherein the bridging moiety is present in an amount of 5*10-10-0.1 Mole bridging moiety/gr nanoparticle.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the bridging moiety of the capture complex comprises a functional group for bonding to an oxide of the nanoparticle and a linking group towards one nitrogen atom of the aromatic moiety of the catalyst entity, and wherein the capture complex is obtained by:
reacting the bridging moiety with the catalyst entity, wherein the linking group of the bridging moiety is functionalized for chemical reaction, which reaction generates the positive charge on the aromatic heterocycle moiety, and generates a combination of the bridging moiety and the catalyst entity;
attachment of the said combination of the bridging moiety and catalyst entity to the nanoparticle by means of physical or chemical bonding.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein the linking group is an alkyl halide.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the nanoparticles are present in the form of aggregates and have an average diameter in a range of 50-200 nm.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the separating step occurs by magnetic separation, centrifugation and/or filtering.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein water is provided to the obtained mixture in order to separate the capture complex from the solvent.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein additives remaining in the mixture after the separation of the capture complex are captured by an active compound.

### Claim 8 (depends on 7)

The method of claim 7, wherein the active compound is carbon black.

### Claim 9 (depends on 1)

The method of claim 1, wherein the captured additive is hydrophobic in nature.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the capture complex is regenerated by removal the additives through washing.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein
the capturing of the additive involves precipitation of the capture complex and the additive,
the separation of the capture complex and the mixture comprises removal of a hydrophilic solution of the solvent and dissolved monomers and dimers;
a washing agent is added to the separated capture complex and the additive is dissolved in the washing agent, and
the capture complex is recovered.

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein the polymer material is a polyester.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein the bridging moiety is one or more of a weak organic acid, silyl comprising groups, and silanol.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein the magnetic particles are at least one of ferromagnetic particles, anti-ferromagnetic particles, ferrimagnetic particles, synthetic magnetic particles, para-magnetic particles, superparamagnetic particles.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the magnetic particles comprise iron oxide.

### Claim 16 (depends on 12)

The method as claimed in claim 12, wherein the polymer material is polyethylene ter-ephthalate (PET) or polyethylene furanoate (PEF), the solvent is ethanediol, the catalyst comprises imidazolium and FeCl4- or Cl-, the bridging moiety is triethoxysilylpropyl or trihydroxysilylpropyl and the nanoparticles is at least one of magnetite, hematite and ma-ghemite.

### Claim 17 (depends on 1)

The method as claimed in claim 1, wherein at least one additive is an organic pigment or a metal-based pigment.

### Claim 18

Method of degrading a mixture of waste polymers comprising polymer material and additives, which additives are released from the waste polymer the additive upon degrada-tion of the polymer material, wherein the polymer material is polyethylene terephthalate (PET) or polyethylene furanoate (PEF), which method comprises the steps of:
providing an improved reusable capture complex;
providing the mixture of waste polymers in solid form in a solvent, wherein the solvent is ethanediol;
degrading the polymer material by glycolysis, wherein the solvent functions as a reactant, and wherein the capture complex catalyses degradation of the polymer material, wherein the additive is released from the polymer and wherein a mixture is obtained;
cooling down the obtained mixture to 50-85° C.;
using the capture complex to capture the additive;
performing a separation to separate the capture complex with the captured additive from the mixture;
cooling the mixture further in order to precipitate a monomer and dimer from the polymer material,
wherein the improved capture complex is not dispersible in water and comprising a catalyst entity, a magnetic nanoparticle of at least one of magnetite, hematite and maghemite, and a bridging moiety chosen from triethoxysilylpropyl or trihydroxysilylpropyl, wherein the catalyst entity and bridging moiety are bonded, and
wherein the bridging moiety and nanoparticle are bonded,
wherein the catalyst entity comprises imidazolium, and a negatively charged moiety chosen from FeCl4- and Cl-.

### Claim 19 (depends on 18)

The method as claimed in claim 18, wherein the nanoparticles are present in the form of aggregates and have an average diameter in a range of 50-200 nm.

### Claim 20 (depends on 19)