# US 10,954,345 B2 · Method of preparing monodispersed polymer polyols

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,345 B2
- Document ID: US10954345B2
- Status: Granted
- Kind: B2
- Application number: 16/291,523
- Filed: 2019-03-04
- Published: 2019-09-05
- Granted: 2021-03-23
- Earliest claimed: 2018-03-02
- Assignees: Korea Kumho Petrochemical Co., Ltd.
- Applicants: Korea Kumho Petrochemical Co., Ltd.
- Inventors: Gi Jung Kim; Seul Gi Kim; Seung Moo Huh
- Web page: https://patentgrep.com/patent/US10954345B2

## CPC

- C08G 18/63: Block or graft polymers obtained by polymerising compounds having carbon-to-carbon double bonds on to polymers
- C08G 81/025: {containing polyether sequences}
- C08F 283/06: on to polyethers, polyoxymethylenes or polyacetals {(C08F283/004 takes precedence)}
- C08G 18/632: {onto polyethers}
- C08G 2101/00: Manufacture of cellular products
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Provided is a method of preparing a polymer polyol including steps of (a) respectively batchwise feeding a polyol and a monomer in a weight ratio of 40 to 60:40 to 60 into a reactor to prepare a mixture; and (b) polymerizing the mixture for 1 to 5 hours to prepare monodispersed particles.

## Claims

### Claim 1

A method of preparing a polymer polyol, comprising the steps of:
(a) respectively batchwise feeding a polyol and a styrene monomer in a weight ratio of 40 to 60:40 to 60 into a reactor to prepare a mixture; and
(b) polymerizing the mixture for 1 to 5 hours to prepare monodispersed particles,
wherein the step (a) further comprises mixing an aqueous solution including a surfactant and dispersing the aqueous solution to convert the mixture into an emulsion.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the polyol is a polyether polyol.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the polyether polyol has a weight average molecular weight of 1,000 to 6,000 g/mol.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the polyether polyol has a hydroxyl value of 30 to 60 mgKOH/g.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the surfactant is a cationic, anionic or nonionic surfactant.

### Claim 6 (depends on 1)

The method according to claim 1, wherein a solvent is further mixed to disperse the mixture in the solvent in the step (a).

### Claim 7 (depends on 6)

The method according to claim 6, wherein the solvent is one selected from the group consisting of toluene, tetrahydrofuran, chloroform, cyclohexane, dioxane, dimethyl sulfoxide, dimethylformamide, acetone, acetonitrile, n-butanol, n-pentanol, chlorobenzene, ethylbenzene, dichloromethane, diethyl ether, tert-butanol, 1,2,-dichloroethylene, diisopropyl ether, ethanol, ethyl acetate, ethyl methyl ketone, heptane, hexane, isopropyl alcohol, isoamyl alcohol, methanol, pentane, n-propyl alcohol, pentachloroethane, 1,1,2,2-tetrachloroethane, 1,1,1-trichloroethane, tetrachlorethylene, tetrachloromethane, trichlorethylene, water, xylene, benzene, nitromethane, and combinations of two or more thereof.