# US 10,954,344 B2 · SiOC-bonded, linear polydimethylsiloxane-polyoxyalkylene block copolymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,344 B2
- Document ID: US10954344B2
- Status: Granted
- Kind: B2
- Application number: 16/456,101
- Filed: 2019-06-28
- Published: 2020-02-20
- Granted: 2021-03-23
- Earliest claimed: 2018-08-15
- Assignees: Evonik Operations GmbH
- Applicants: Evonik Operations GmbH
- Inventors: Wilfried Knott; Horst Dudzik; Dagmar Windbiel
- Web page: https://patentgrep.com/patent/US10954344B2

## CPC

- C08G 77/14: containing silicon bound to oxygen-containing groups
- C08G 77/46: containing polyether sequences
- C08G 18/61: Polysiloxanes
- C08G 77/70: {Siloxanes defined by use of the MDTQ nomenclature}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The production of SiOC-bonded, linear polydimethylsiloxane-polyoxyalkylene block copolymers comprising repeating (AB) units by reaction of polyether diols with trifluoromethanesulfonic acid-acidified, equilibrated α,ω-diacetoxypolydimethylsiloxanes is described, wherein the reaction is undertaken by adding a solid, liquid or gaseous base, optionally using inert solvents.

## Claims

### Claim 1

A process for producing SiOC-bonded, linear polydimethylsiloxane-polyoxyalkylene block copolymers comprising repeating (AB) units by reaction of polyether diols with trifluoromethanesulfonic acid-acidified, end-equilibrated α,ω-diacetoxypolydimethylsiloxanes, wherein the reaction is undertaken by adding a solid, liquid or gaseous base, and using inert solvents.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the molar ratio of trifluoromethanesulfonic acid-acidified, end-equilibrated α,ω-diacetoxypolydimethylsiloxanes to polyether diols is in the range from 0.90 to 1.10.

### Claim 3 (depends on 2)

The process according to claim 2, wherein the base is selected from the group consisting of alkali metal and/or alkaline earth metal carbonates and/or hydrogencarbonates, and/or amines.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the reaction is performed at temperatures of 20° C. to 120° C.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the bases are selected from the group consisting of alkali metal and/or alkaline earth metal carbonates and/or hydrogencarbonates and/or amines.

### Claim 6 (depends on 1)

The process according to claim 1, wherein inert solvents are selected from the group consisting of alkanes, cycloalkanes, alkylaromatics, end-capped polyethers and/or emollient esters, the esters derived from lauric acid, myristic acid, palmitic acid, stearic acid, oleic acid, isostearic acid, ricinoleic acid and behenic acid combined with cetyl, stearyl, isostearyl, oleyl, octyldodecyl, myristyl and behenyl alcohol or glycerol.

### Claim 7 (depends on 1)

The process according to claim 1, wherein the weight-average molecular weight of each siloxane block (A), (—(CH3)2SiO—)b, is between 600 and 6100 g/mol.

### Claim 8 (depends on 1)

The process according to claim 1, wherein the polyoxyalkylene block (B), (—CnH(2n-1)R1mO—)c, wherein R1 represents methyl, contains mixed oxyethylene and oxypropylene units having an oxyethylene proportion of from 30 to 70 percent by weight and an oxypropylene proportion of from 70 to 30 percent by weight based on the total content of oxyalkylene units in the block.

### Claim 9 (depends on 1)

The process according to claim 1, wherein the weight-average molecular weight of each polyoxyalkylene block (B), (CnH(2n-1)R1mO)c, wherein R1 represents methyl, is between 600 and 10 000 g/mol.

### Claim 10 (depends on 1)

The process according to claim 1, wherein the proportion of the siloxane blocks A in the total copolymer is between 20 and 50, percent by weight.

### Claim 11 (depends on 1)

The process according to claim 1, wherein the polydimethylsiloxane-polyoxyalkylene block copolymer has a weight-average molecular weight of 10 000 g/mol to 200 000 g/mol.

### Claim 12 (depends on 1)

The process according to claim 1, wherein the molar ratio of trifluoromethanesulfonic acid-acidified, end-equilibrated α,ω-diacetoxypolydimethylsiloxanes to polyether diols is in the range from 0.95 to 1.05.

### Claim 13 (depends on 1)

The process according to claim 1, wherein the reaction is performed at temperatures of 20° C. to 70° C.

### Claim 14 (depends on 1)

The process according to claim 1, wherein the base is gaseous ammonia.

### Claim 15 (depends on 1)

The process according to claim 1, wherein the inert solvent is myristyl myristate.

### Claim 16 (depends on 1)

The process according to claim 1, wherein the proportion of the siloxane blocks A in the total copolymer is between 25 and 40 percent by weight.

### Claim 17 (depends on 1)

The process according to claim 1, wherein the polydimethylsiloxane-polyoxyalkylene block copolymer has a weight-average molecular weight of 25,000 g/mol to 180,000 g/mol.

### Claim 18 (depends on 1)

The process according to claim 1, wherein the polydimethylsiloxane-polyoxyalkylene block copolymer has a weight-average molecular weight of 40,000 g/mol to 140,000 g/mol.