# US 10,954,314 B2 · Method of disintegrating pulp for use in cellulose acetate production and method of producing cellulose acetate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,314 B2
- Document ID: US10954314B2
- Status: Granted
- Kind: B2
- Application number: 15/323,928
- Filed: 2014-07-14
- Published: 2017-05-25
- Granted: 2021-03-23
- Earliest claimed: 2014-07-14
- Assignees: Daicel Corporation
- Applicants: Daicel Corporation
- Inventors: Mitsuteru Hosaka; Toshinori Okano; Yuji Ida
- Web page: https://patentgrep.com/patent/US10954314B2

## CPC

- C08B 3/06: Cellulose acetate {, e.g. mono-acetate, di-acetate or tri-acetate}
- B02C 7/06: with horizontal axis (B02C7/04 takes precedence)
- B02C 19/06: Jet mills
- B02C 19/061: {of the cylindrical type (B02C19/068 takes precedence)}
- C08B: POLYSACCHARIDES; DERIVATIVES THEREOF (polysaccharides containing less than six saccharide radicals attached to each other by glycosidic linkages C07H; fermentation or enzyme-using processes C12P19/00; sugar industry C13; production of cellulose D21)
- B02C: CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL; MILLING GRAIN ({household tools and machines for pulverising foodstuffs, e.g. coffee and spice mills A47J42/00; pharmaceutical mortars A61J3/02; mechanical processing of refuse and garbage B03B9/06; dressing mould materials by grinding B22C5/04}; obtaining metallic powder by crushing, grinding or milling B22F9/04; {recovery of plastics by disintegrating B29B17/00; crushing raw materials in starch making C08B30/02; beaters for papermaking D21D1/02; crushing devices specially for transport in mines E21F13/002; slag crushing devices F23J1/00; fuel milling devices in combustion apparatus F23K1/00; household devices for crushing coal F24B15/02; ice disintegrating devices F25C5/02})

## Abstract

A method of disintegrating pulp for use in cellulose acetate production includes: a primary disintegration step of disintegrating a pulp sheet into pulp pieces having an average area of not more than 45 cm2; and a secondary disintegration step of disintegrating the pulp pieces with an impact shock exerted by a jet mill (20). The jet mill (20) includes: a cylindrical casing (21) provided with an inlet (21d) and an outlet (21e); and a rotor (25) including a plurality of blades (25a) provided on its outer peripheral portion, the plurality of blades (25a) facing an inner peripheral surface of the casing (21).

## Claims

### Claim 1

A method of producing cellulose acetate, comprising a disintegration step including:
a primary disintegration step of disintegrating a pulp sheet, to which water has not been added, into pulp pieces having an average area of not more than 45 cm2 by a disc refiner or a hammer mill; and
a secondary disintegration step of disintegrating the pulp pieces with an impact shock exerted by a jet mill, wherein the jet mill includes a cylindrical casing provided with an inlet and an outlet and a rotor including a plurality of blades provided on its outer peripheral portion, the plurality of blades facing an inner peripheral surface of the casing;
a pretreatment step of performing a pretreatment of adding acetic acid to pulp that has been disintegrated by the disintegration step; and
an acetylation step of adding acetic acid, acetic anhydride, and a sulfuric acid catalyst to the pulp that has undergone the pretreatment step, and subjecting a resulting mixture to acetylation while controlling a temperature of the mixture;
wherein the cellulose acetate has a lower proportion of matter insoluble in a 96% aqueous acetone at 50° C. when compared to a cellulose acetate produced by an otherwise identical method wherein the secondary disintegration is carried out by a disc refiner.

### Claim 2

A method of producing cellulose acetate, consisting essentially of a disintegration step including:
a primary disintegration step of disintegrating a pulp sheet, to which water has not been added, into pulp pieces having an average area of not more than 45 cm2 by a disc refiner or a hammer mill; and
a secondary disintegration step of disintegrating the pulp pieces with an impact shock exerted by a jet mill, wherein the jet mill includes a cylindrical casing provided with an inlet and an outlet and a rotor including a plurality of blades provided on its outer peripheral portion, the plurality of blades facing an inner peripheral surface of the casing;
a pretreatment step of performing a pretreatment of adding acetic acid to pulp that has been disintegrated by the disintegration step; and
an acetylation step of adding acetic acid, acetic anhydride, and a sulfuric acid catalyst to the pulp that has undergone the pretreatment step, and subjecting a resulting mixture to acetylation while controlling a temperature of the mixture.