# US 10,954,164 B2 · Formed hexagonal boron nitride body, heat-treated hexagonal boron nitride body and processes for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,164 B2
- Document ID: US10954164B2
- Status: Granted
- Kind: B2
- Application number: 16/323,454
- Filed: 2017-07-21
- Published: 2019-06-13
- Granted: 2021-03-23
- Earliest claimed: 2016-08-05
- Assignees: 3M Innovative Properties Company
- Applicants: 3M Innovative Properties Company
- Inventors: Jan C. Zimmer; Ursula Kayser; Krishna B. Uibel; Christoph Lesniak
- Web page: https://patentgrep.com/patent/US10954164B2

## CPC

- C04B 35/583: based on boron nitride
- C04B 35/103: containing non-oxide refractory materials, e.g. carbon (C04B35/106 takes precedence)
- C04B 35/62695: {Granulation or pelletising (devices for shaping artificial aggregates from ceramic mixtures B28B1/004)}
- C04B 2235/3201: Alkali metal oxides or oxide-forming salts thereof
- C04B 2235/3205: Alkaline earth oxides or oxide forming salts thereof, e.g. beryllium oxide
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/321: Dolomites, i.e. mixed calcium magnesium carbonates
- C04B 2235/3218: Aluminium (oxy)hydroxides, e.g. boehmite, gibbsite, alumina sol
- C04B 2235/3409: Boron oxide, borates, boric acids, or oxide forming salts thereof, e.g. borax
- C04B 2235/386: Boron nitrides
- C04B 2235/442: Carbonates
- C04B 2235/5292: Flakes, platelets or plates
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/61: Mechanical properties, e.g. fracture toughness, hardness, Young's modulus or strength
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/767: Hexagonal symmetry, e.g. beta-Si3N4, beta-Sialon, alpha-SiC or hexa-ferrites
- C04B 2235/77: Density
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Provided are materials for a formed body comprising hexagonal boron nitride and such formed bodies. Also provided are heat-treated formed body obtained by heat-treating the formed bodies. The invention further relates to processes for making the formed body and the heat-treated formed body.

## Claims

### Claim 1

A formed body comprising a material composition, the material composition comprising hexagonal boron nitride, a water-soluble boron compound selected from the group consisting of boric acid (H3BO3) and ammonium borates, and boehmite, wherein as expressed as a molar ratio of AlO(OH): H3BO3, the molar ratio of boehmite to the water-soluble boron compound is from 0.3:1 to 6:1, wherein the boehmite is able to split off a gaseous phase at a heat treatment at a temperature of at most 1000° C., and is able to form, with the water-soluble boron compound, a water-insoluble boron compound at a heat treatment at a temperature of 200-1000° C.;
wherein the gaseous phase is water, carbon dioxide, or a combination thereof.

### Claim 2 (depends on 1)

The formed body of claim 1, wherein the content of the boehmite in the material composition is at least 0.5% by weight, based on the total weight of the formed body.

### Claim 3 (depends on 1)

The formed body of claim 1, wherein the molar ratio of boehmite to the water soluble boron compound in the material composition is from 1:1 to 2:1 expressed as a molar ratio of AlO(OH):H3B03.

### Claim 4 (depends on 1)

The formed body of claim 1, wherein the boron nitride content is at least 15% by weight, based on the total weight of the material composition.

### Claim 5 (depends on 1)

The formed body according to claim 1, wherein the formed body has a compressive strength of at least 4 N/mm2, wherein the compressive strength is measured as a maximum force before rupture of a test sample of the formed body, divided by the area of the test sample on which the load is applied.

### Claim 6 (depends on 1)

The formed body according to claim 1, wherein the formed body has a Brinell hardness of at least 2 HBW 2.5/2, wherein the Brinell hardness is measured according to DIN EN ISO 6506-1-2013.

### Claim 7

A process of making a formed body, wherein the process comprises the steps
(a) providing a first powder comprising hexagonal boron nitride powder;
(b) obtaining a second powder comprising the hexagonal boron nitride powder and at least one water-soluble boron compound selected from the group consisting of boric acid (H3BO3) and ammonium borates, by at least one of:
(i) generating the at least one water soluble boron compound by mechanically pre-treating the powder of step (a) and
(ii) by adding the at least one water-soluble boron compound to the powder provided in step (a);
(c) adding boehmite to the second powder of step (b), wherein as expressed as a molar ratio of AlO(OH): H3BO3, the molar ratio of boehmite to the water-soluble boron compound is from 0.3:1 to 6:1 ;
(d) mixing the second powder of step (b) and the boehmite added in step (c), thereby obtaining a material composition comprising hexagonal boron nitride;
(e) optionally granulating the material composition of step (d), thereby obtaining a material composition comprising hexagonal boron nitride, wherein the material composition is granulated; and
(f) forming the material composition of step (d) or the material composition of step (e) into a shape.

### Claim 8

A process for making a heat-treated formed body, wherein the process comprises the steps
(a) providing a first powder comprising hexagonal boron nitride powder;
(b) obtaining a second powder comprising hexagonal boron nitride powder and at least one water-soluble boron compound selected from the group consisting of boric acid (H3BO3) and ammonium borates, by at least one of:
(i)generating the at least one water soluble boron compound by mechanically pre-treating the first powder of step (a) and
(ii) by adding the at least one water-soluble boron compound to the first powder provided in step (a), thereby;
(c) adding boehmite to the second powder of step (b), wherein as expressed as a molar ratio of AlO(OH):
H3BO3, the molar ratio of boehmite to the water-soluble boron compound is from 0.3:1 to 6:1 the further inorganic compound;
(d) mixing the second powder of step (b) and the boehmite added in step (c), thereby obtaining a material composition comprising hexagonal boron nitride;
(e) optionally granulating the material composition of step (d), thereby obtaining a material composition comprising hexagonal boron nitride, wherein the material composition is granulated; and
(f) forming the material composition of step (d) or the material composition of step (e) into a shape, thereby obtaining a formed body; and
(g) heat-treating the formed body of step (f) at a temperature of from 200 to 1000° C.

### Claim 9 (depends on 8)

A heat-treated formed body obtained by the process of claim 8, wherein the heat-treated formed body comprises hexagonal boron nitride and the reaction product between the water-soluble boron compound and boehmitem, and wherein the reaction product is a water-insoluble boron compound.

### Claim 10 (depends on 9)

The heat-treated formed body according to claim 9, wherein the reaction product between the water-soluble boron compound and boehmite is aluminum borate Al4B2O9.

### Claim 11 (depends on 9)

The heat-treated formed body according to claim 9, wherein the compressive strength of the heat-treated formed body is at least 4 N/mm2, wherein the compressive strength is measured as maximum force before rupture of a test sample of the formed body, divided by the area of the test sample on which the load is applied.

### Claim 12 (depends on 9)

The heat-treated formed body according to claim 9, wherein the heat-treated formed body has a Brinell hardness of at least 3 HBW 2.5/2, wherein the Brinell hardness is measured according to DIN EN ISO 6506-1-2013.

### Claim 13 (depends on 9)

The heat-treated formed body according to claim 9, wherein the heat-treated formed body has a boron nitride content of at least 15% by weight, based on the total weight of the heat-treated formed body.