# US 10,954,163 B2 · Lightweight high-strength ceramsite and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,163 B2
- Document ID: US10954163B2
- Status: Granted
- Kind: B2
- Application number: 16/464,878
- Filed: 2017-05-21
- Published: 2019-10-24
- Granted: 2021-03-23
- Earliest claimed: 2016-12-16
- Assignees: Guangdong Tsingda Tongke Environmental Protection Technology Co., Ltd.
- Applicants: Guangdong Tsingda Tongke Environmental Protection Technology Co., Ltd.
- Inventors: Yihai Jia; Xihong Wang; Siying Chen; Chuanxing Wang
- Web page: https://patentgrep.com/patent/US10954163B2

## CPC

- C04B 33/04: Clay; Kaolin
- C04B 33/1305: {Organic additives}
- C04B 33/131: {Inorganic additives}
- C04B 33/1315: {Non-ceramic binders}
- C04B 33/132: Waste materials; Refuse {; Residues} (C04B33/16 takes precedence)
- C04B 33/1322: {Red mud}
- C04B 33/1352: {Fuel ashes, e.g. fly ash}
- C04B 33/138: from metallurgical processes, e.g. slag, furnace dust, galvanic waste
- C04B 33/30: Drying methods
- C04B 33/32: Burning methods
- C04B 35/18: rich in aluminium oxide
- C04B 35/62204: {using waste materials or refuse (clay-wares containing waste materials C04B33/132)}
- C04B 35/62695: {Granulation or pelletising (devices for shaping artificial aggregates from ceramic mixtures B28B1/004)}
- C04B 35/6316: {Binders based on silicon compounds}
- C04B 35/632: Organic additives
- C04B 35/6365: {Cellulose or derivatives thereof}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 2235/3201: Alkali metal oxides or oxide-forming salts thereof
- C04B 2235/3203: Lithium oxide or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/3427: Silicates other than clay, e.g. water glass
- C04B 2235/3463: Alumino-silicates other than clay, e.g. mullite
- C04B 2235/349: Clays, e.g. bentonites, smectites such as montmorillonite, vermiculites or kaolines, e.g. illite, talc or sepiolite
- C04B 2235/36: Glass starting materials for making ceramics, e.g. silica glass
- C04B 2235/606: Drying
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/77: Density
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- Y02P 40/60: Production of ceramic materials or ceramic elements, e.g. substitution of clay or shale by alternative raw materials, e.g. ashes
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A lightweight high-strength ceramsite, comprising solid raw materials and activator as the raw materials, which can be respectively expressed in parts by weight, the solid raw materials: 100 parts, the activator: 1-15 parts; wherein said solid raw materials comprise fly ash: 100 parts, high-alumina fly ash, bauxite and red mud: 6-18 parts, silica fume: 1-5 parts, surfactant: 0.1-3 parts, plasticizer: 6-24 parts; and said activator comprises alkali metal hydroxide: 5-20 parts and alkali metal silicate: 80-95 parts. The lightweight high-strength ceramsite product prepared has a density level of 700-1100 kg/m3 and cylindrical compressive strength of 10-20 MPa, and thus is not susceptible to damage.

## Claims

### Claim 1

A lightweight high-strength ceramsite, comprising solid raw materials and solid activator as raw materials, which can be respectively expressed in parts by weight, the solid raw materials:100 parts, the activator: 1-15 parts, characterized in that said solid raw materials comprise fly ash: 100 parts, high-alumina fly ash, bauxite and red mud: 6-18 parts, silica fume: 1-5 parts, surfactant: 0.1-3 parts, plasticizer: 6-24 parts; and said activator comprises alkali metal hydroxide: 5-20 parts and 60-95% by weight of alkali metal silicate solution: 80-95 parts.

### Claim 2 (depends on 1)

The lightweight high-strength ceramsite according to claim 1, characterized in that said fly ash comprises the following components, loss on ignition: 2-10%, SiO2: 30%-70%, Al2O3:10%-50%, CaO: 1%-15%, Fe2O3: 1%-18%, MgO: 0.01%-8%, and TiO2: 0.01%-3%.

### Claim 3 (depends on 1)

The lightweight high-strength ceramsite according to claim 1, characterized in that said plasticizer is one or more selected from the group consisting of Guangdong white clay, Guangdong black clay, kaolin, bentonite, PVA, and cellulose.

### Claim 4 (depends on 1)

The lightweight high-strength ceramsite according to claim 1, characterized in that said high-alumina fly ash and bauxite comprise an alumina content of not less than 37%; and the weight ratio of red mud to high-alumina fly ash and bauxite is 1:2-5.

### Claim 5 (depends on 1)

The lightweight high-strength ceramsite according to claim 1, characterized in that said solid raw materials further comprise iron ore tailings: 0.01-5 parts and calcite: 0.01-5 parts.

### Claim 6 (depends on 1)

The lightweight high-strength ceramsite according to claim 1, characterized in that said alkali metal hydroxide is one or more selected from the group consisting of sodium hydroxide, potassium hydroxide and lithium hydroxide; and said alkali metal silicate in the alkali metal silicate solution is one or more selected from the group consisting of sodium silicate, potassium silicate and lithium silicate.

### Claim 7 (depends on 1)

The lightweight high-strength ceramsite according to claim 1, characterized in that said surfactant is sodium lignosulfonate.

### Claim 8 (depends on 1)

A method for preparing lightweight high-strength ceramsite, characterized in comprising the following steps:
a. Weighing solid raw materials comprising fly ash: 100 parts, high-alumina fly ash, bauxite and red mud: 6-18 parts, silica fume: 1-5 parts, surfactant: 0.1-3 parts, plasticizer: 6-24 parts, and mixing the same, and preparing a solid activator: dissolving alkali metal hydroxide in an alkali metal silicate solution, after cooling to room temperature, stirring until a small amount of white precipitates are observed, pouring the resulting solution into a clean container; white crystals are formed at room temperature for 1-20 minutes into agglomerates, which are pulverized to form the solid activator;
b. Mixing: mixing the solid raw materials and the solid activator thoroughly to form mixed materials;
c. Pelletizing: pelletizing the mixed materials into particles;
d. Curing: maintaining the particles under the conditions with a temperature of 70-100° C. and a humidity of 70-90% for 1-2 hours to be cured;
e. Drying: drying the cured particles at a temperature of 100-300° C.;
f. Sintering: subjecting the dried particles to a predetermined sintering process for 60-90 min;
g. Forming finished product: cooling the sintered particles to room temperature to yield a lightweight high-strength ceramsite according to claim 1.

### Claim 9 (depends on 8)

The method for preparing lightweight high-strength ceramsite according to claim 8, characterized in that the sintering process comprises specific steps of elevating the temperature from 100-300° C. at a rate of 20-40° C./min to 500-700° C., and subsequently further elevating the temperature to 1050-1350° C. at a rate of 5-25° C./min.