# US 10,954,154 B2 · Shaped glass laminates and methods for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,154 B2
- Document ID: US10954154B2
- Status: Granted
- Kind: B2
- Application number: 15/899,689
- Filed: 2018-02-20
- Published: 2018-08-23
- Granted: 2021-03-23
- Earliest claimed: 2017-02-20
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Michele Marie-Louise Fredholm
- Web page: https://patentgrep.com/patent/US10954154B2

## CPC

- C03B 23/0252: {by gravity only, e.g. sagging (C03B23/035 takes precedence)}
- B32B 17/10036: {comprising two outer glass sheets}
- B32B 17/10082: {Properties of the bulk of a glass sheet}
- B32B 17/101: {having a predetermined coefficient of thermal expansion [CTE]}
- B32B 17/1011: {having predetermined tint or excitation purity}
- B32B 17/10119: {having a composition deviating from the basic composition of soda-lime glass, e.g. borosilicate}
- B32B 17/10137: {Chemical strengthening}
- B32B 17/10761: {containing vinyl acetal}
- B32B 17/1077: {containing polyurethane}
- B32B 17/10788: {containing ethylene vinylacetate}
- B32B 17/10889: {shaping the sheets, e.g. by using a mould (B32B17/10816 takes precedence)}
- B60J 1/008: {of special shape, e.g. beveled edges, holes for attachment, bent windows, peculiar curvatures such as when being integrally formed with roof, door, etc.}
- C03B 23/025: by gravity
- C03B 23/03: by press-bending between shaping moulds
- C03B 23/0357: {by suction without blowing, e.g. with vacuum or by venturi effect}
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- B32B 2250/03: 3 layers
- B32B 2250/40: Symmetrical or sandwich layers, e.g. ABA, ABCBA, ABCCBA
- B32B 2605/006: Transparent parts other than made from inorganic glass, e.g. polycarbonate glazings
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B60J: WINDOWS, WINDSCREENS, NON-FIXED ROOFS, DOORS, OR SIMILAR DEVICES FOR VEHICLES; REMOVABLE EXTERNAL PROTECTIVE COVERINGS SPECIALLY ADAPTED FOR VEHICLES (fastening, suspending, closing, or opening of such devices E05)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Embodiments of a laminate including a first curved glass substrate comprising a first viscosity (poises) at a temperature of 630° C.; a second curved glass substrate comprising a second viscosity that is greater than the first viscosity at a temperature of 630° C.; and an interlayer disposed between the first curved glass substrate and the second curved glass substrate, are disclosed. In one or more embodiments, the first curved glass substrate exhibits a first sag depth that is within 10% of a second sag depth of the second curved glass substrate. In one or more embodiments, the first glass substrate and the second glass substrate exhibit a shape deviation therebetween of about ±5 mm or less as measured by an optical three-dimensional scanner or exhibit minimal optical distortion. Embodiments of vehicles including such laminates and methods for making such laminates are also disclosed.

## Claims

### Claim 1

A laminate comprising:
a first curved glass substrate comprising a first major surface, a second major surface opposing the first major surface, a first thickness defined as a distance between the first major surface and the second major surface, a first sag depth of about 2 mm or greater, and the first curved glass substrate comprising a first viscosity;
a second curved glass substrate comprising a third major surface, a fourth major surface opposing the third major surface, a second thickness defined as a distance between the third major surface and the fourth major surface, a second sag depth of about 2 mm or greater, and the second curved glass substrate comprising a second viscosity that is greater than the first viscosity at a temperature of 630° C.; and
an interlayer disposed between the first curved glass substrate and the second curved glass substrate and adjacent the second major surface and the third major surface,
wherein the first sag depth is within 10% of the second sag depth and a shape deviation between the first glass substrate and the second glass substrate is ±5 mm or less as measured by an optical three-dimensional scanner,
wherein the laminate comprises an effective viscosity that is between the first viscosity and the second viscosity at a temperature (T) in a range from about 500° C. to about 700° C., and is determined by the equation: μeff(T)=((μ1(T)t1)/(t1+t2))+((μ2(T)t2)/(t1+t2)), where μ1(T) is the viscosity of the first curved glass substrate at temperature (T), t1 is the thickness of the first curved glass substrate, μ2(T) is the viscosity of the second curved glass substrate at temperature (T), t2 is the thickness of the second curved glass substrate,
wherein one of or both the first major surface or the fourth major surface exhibits an optical distortion of less than 200 millidiopters as measured by an optical distortion detector using transmission optics according to ASTM 1561, and
wherein the first major surface or the second major surface comprises a membrane tensile stress of less than 7 MPa as measured by a surface stressmeter, according to ASTM C1279.

### Claim 2 (depends on 1)

The laminate of claim 1, wherein, at a temperature of about 630° C., the second viscosity is in a range from about 10 times the first viscosity to about 750 times the first viscosity.

### Claim 3 (depends on 1)

The laminate of claim 1, wherein the second thickness is less than the first thickness.

### Claim 4 (depends on 1)

The laminate of claim 1, wherein the first curved glass substrate comprises a first sag temperature and the second curved glass substrate comprises a second sag temperature that differs from the first sag temperature and wherein a difference between the first sag temperature and the second sag temperature is in a range from about 30° C. to about 150° C.

### Claim 5 (depends on 1)

The laminate of claim 1, wherein the second sag depth is in a range from about 5 mm to about 30 mm.

### Claim 6 (depends on 1)

The laminate of claim 1, wherein the laminate is substantially free of visual distortion as measured by ASTM C1652/C1652M.

### Claim 7 (depends on 1)

The laminate of claim 1, wherein one of or both the first curved glass substrate or the second curved glass substrate comprises a compressive stress region and a central tension region formed by a coefficient of thermal expansion difference between portions of the corresponding curved glass substrate that mechanically strengthens the corresponding curved glass substrate.

### Claim 8

A vehicle comprising:
a body defining an interior and an opening in communication with the interior;
a complexly-curved laminate disposed in the opening, the complexly-curved laminate comprising:
a first curved glass substrate comprising a first major surface, a second major surface opposing the first major surface, a first thickness defined as a distance between the first major surface and the second major surface, and a first sag depth of about 2 mm or greater, the first curved glass substrate comprising a first viscosity;
a second curved glass substrate comprising a third major surface, a fourth major surface opposing the third major surface, a second thickness defined as a distance between the third major surface and the fourth major surface, a second sag depth of about 2 mm or greater, and the second curved glass substrate comprising a second viscosity that is greater than the first viscosity at a temperature of about 630° C.; and
an interlayer disposed between the first curved glass substrate and the second curved glass substrate and adjacent the second major surface and the third major surface,
wherein the first sag depth is within 10% of the second sag depth and a shape deviation between the first curved glass substrate and the second curved glass substrate is ±5 mm or less as measured by an optical three-dimensional scanner,
wherein the laminate comprises an effective viscosity that is between the first viscosity and the second viscosity at a temperature (T) in a range from about 500° C. to about 700° C., and is determined by the equation: μeff(T)=((μ1(T)t1)/(t1+t2))+((μ2(T)t2)/(t1+t2)), where μ1(T) is the viscosity of the first curved glass substrate at temperature (T), t1 is the thickness of the first curved glass substrate, μ2(T) is the viscosity of the second curved glass substrate at temperature (T), t2 is the thickness of the second curved glass substrate,
wherein one of or both the first major surface or the fourth major surface exhibits an optical distortion of less than 200 millidiopters as measured by an optical distortion detector using transmission optics according to ASTM 1561, and
wherein the first major surface or the second major surface comprises a membrane tensile stress of less than 7 MPa as measured by a surface stressmeter, according to ASTM C1279.

### Claim 9 (depends on 8)

The vehicle of claim 8, wherein, at a temperature of 630° C., the second viscosity is in a range from about 10 times the first viscosity to about 750 times the first viscosity.

### Claim 10 (depends on 8)

The vehicle of claim 8, wherein the second thickness is less than the first thickness.

### Claim 11 (depends on 8)

The vehicle of claim 8, wherein the first curved glass substrate comprises a first sag temperature and the second curved glass substrate comprises a second sag temperature that differs from the first sag temperature.

### Claim 12 (depends on 8)

The vehicle of claim 8, wherein the laminate is substantially free of visual distortion as measured by ASTM C1652/C1652M.

### Claim 13 (depends on 8)

The laminate of claim 8, wherein one of or both the first curved glass substrate or the second curved glass substrate comprises a compressive stress region and a central tension region formed by a coefficient of thermal expansion difference between portions of the corresponding curved glass substrate that mechanically strengthens the corresponding curved glass substrate.

### Claim 14 (depends on 1)

A method of forming the curved laminate of claim 1, the method comprising:
forming a stack comprising a first glass substrate and a second glass substrate, the first glass substrate comprising the first viscosity and a first sag temperature, the second glass substrate comprising the second viscosity greater than the first viscosity at a temperature of 630° C. and a second sag temperature that differs from the first sag temperature; and
heating the stack and co-shaping the stack to form a co-shaped stack, the co-shaped stack comprising the first curved glass substrate having the first sag depth and the second curved glass substrate having the second sag depth, the first curved glass substrate formed from the first glass substrate, and the second curved glass substrate formed from the second glass substrate.

### Claim 15 (depends on 14)

The method of claim 14, wherein one of or both the first curved glass substrate or the second curved glass substrate comprises a compressive stress region and a central tension region formed by a coefficient of thermal expansion difference between portions of the corresponding curved glass substrate that mechanically strengthens the corresponding curved glass substrate.

### Claim 16 (depends on 14)

The method of claim 14, wherein the second glass substrate is disposed on the first glass substrate or the first glass substrate is disposed on the second glass substrate.

### Claim 17 (depends on 14)

The method of claim 14, wherein heating the stack comprises heating the stack to a temperature different from the first sag temperature and the second sag temperature, heating the stack to a temperature between the first sag temperature and the second sag temperature, or heating the stack to the first sag temperature or the second sag temperature.

### Claim 18 (depends on 14)

The method of claim 14, further comprising placing the stack on a female mold and heating the stack on the female mold, wherein co-shaping the stack comprises sagging the stack through an opening in the female mold using gravity.

### Claim 19 (depends on 18)

The method of claim 18, further comprising applying a vacuum to the stack to facilitate co-shaping the stack.

### Claim 20 (depends on 14)

The method of claim 14, further comprising generating a vacuum force between the first glass substrate and the second glass substrate.

### Claim 21 (depends on 14)

The method of claim 14, further comprising forming a temporary bond between the first glass substrate and the second glass substrate, wherein the temporary bond comprises a vacuum force.

### Claim 22 (depends on 14)

The method of claim 14, further comprising inserting an interlayer between the first curved glass substrate and the second curved glass substrate, and laminating the first curved glass substrate, the interlayer, and the second curved glass substrate together.