# US 10,953,633 B2 · Strengthened thin glass-polymer laminates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,953,633 B2
- Document ID: US10953633B2
- Status: Granted
- Kind: B2
- Application number: 14/423,956
- Filed: 2013-08-27
- Published: 2015-09-17
- Granted: 2021-03-23
- Earliest claimed: 2012-08-31
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Kiat Chyai Kang; Govindarajan Natarajan; Yu Xiao
- Web page: https://patentgrep.com/patent/US10953633B2

## CPC

- B32B 17/10: of synthetic resin
- B29C 65/02: by heating, with or without pressure
- B29C 65/54: between pre-assembled parts
- B29C 66/7465: {Glass}
- B29C 66/81261: {Thermal properties, e.g. thermal conductivity, thermal expansion coefficient}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- B32B 17/10018: {comprising only one glass sheet}
- B32B 17/10036: {comprising two outer glass sheets}
- B32B 17/101: {having a predetermined coefficient of thermal expansion [CTE]}
- B32B 17/10743: {containing acrylate (co)polymers or salts thereof}
- B32B 17/10752: {containing polycarbonate}
- B32B 27/06: as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a layer of a particular substance B32B9/045; next to a bituminous or tarry layer B32B11/046; next to a water setting substance layer B32B13/12; next to a metal layer B32B15/08; next to a glass layer B32B17/10; next to a layer formed of natural mineral fibres or particles B32B19/045; next to a wood layer B32B21/08; next to a cellulosic plastic layer B32B23/08; next to a natural or synthetic rubber layer B32B25/08)}
- B32B 27/308: {comprising acrylic (co)polymers}
- B32B 37/06: characterised by the heating method
- B32B 37/08: characterised by the cooling method
- B32B 37/144: {using layers with different mechanical or chemical conditions or properties, e.g. layers with different thermal shrinkage, layers under tension during bonding (constructional features for tensioning B32B38/1825)}
- B32B 38/0012: {Mechanical treatment, e.g. roughening, deforming, stretching}
- B29K 2105/0097: {Glues or adhesives, e.g. hot melts or thermofusible adhesives}
- B29K 2105/253: {Preform}
- B29K 2833/12: Polymers of methacrylic acid esters, e.g. PMMA, i.e. polymethylmethacrylate
- B29K 2909/08: Glass
- B29K 2995/0026: Transparent
- B29L 2009/00: Layered products
- B29L 2031/3412: {Insulators}
- B32B 37/12: characterised by using adhesives
- B32B 2250/02: 2 layers
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2309/02: Temperature
- B32B 2309/12: Pressure
- B32B 2315/08: Glass
- B32B 2457/00: Electrical equipment
- Y10T 428/24628: Nonplanar uniform thickness material
- Y10T 428/266: of base or substrate
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A glass-polymer laminate structure includes a flexible glass substrate having a thickness of no more than about 0.3 mm. A polymer layer is laminated to a surface of the flexible glass substrate having a coefficient of thermal expansion (CTE) that is at least about 2 times a CTE of the flexible glass substrate. The polymer layer is laminated to the surface of the flexible glass substrate after thermally expanding the polymer layer to provide the flexible glass substrate with an in-plane compressive stress of at least about 30 MPa along a thickness of the flexible glass substrate.

## Claims

### Claim 1

A thermally bent, asymmetric glass-polymer laminate structure comprising:
a flexible glass substrate having a thickness of no more than about 0.3 mm;
a polymer layer laminated to a first surface of the flexible glass substrate, and
an adhesive layer that laminates the polymer layer to the flexible glass substrate wherein the polymer layer has a coefficient of thermal expansion (CTE) that is at least 2 times a CTE of the flexible glass substrate, or has a CTE that is at least 3 ppm/° C. greater than a CTE of the flexible glass substrate,
and wherein the polymer layer is laminated to the first surface of the flexible glass substrate using the adhesive that sets only after thermally expanding the polymer layer at an elevated temperature of greater than 20° C. and less than the softening temperature of the polymer to bond the polymer layer to the flexible glass substrate while thermally expanded to provide the flexible glass substrate with a thermally bent configuration that is bent toward the polymer layer when the polymer layer is controllably cooled at a rate of less than or equal to 1-2° C./minute thereby reducing a tensile stress in the flexible glass substrate due to the bent configuration;
wherein the flexible glass substrate has a compressive stress of greater than about 30 MPa at the first surface and a tensile stress of less than about 40 MPa at a second surface that is opposite the first surface.

### Claim 2 (depends on 1)

The laminate structure of claim 1, wherein the flexible glass substrate has a compressive stress of at least about 80 MPa across the thickness of the flexible glass substrate.

### Claim 3 (depends on 1)

The laminate structure of claim 1, wherein the polymer layer has a CTE that is at least about 10 times the CTE of the flexible glass substrate.

### Claim 4 (depends on 1)

The glass-polymer laminate structure of claim 1, further comprising a first polymer layer and a second polymer layer wherein the flexible glass substrate layer is placed between the first polymer layer and the second polymer layer.

### Claim 5 (depends on 4)

The glass-polymer laminate structure of claim 4, wherein in-plane compressive stresses generated across a thickness of the flexible glass substrate layer are compensated by tensile stresses in the first polymer layer and the second polymer layer.

### Claim 6 (depends on 1)

The glass-polymer laminate structure of claim 1, further comprising a first flexible glass substrate layer and a second flexible glass substrate layer, wherein the polymer layer is placed between the first flexible glass substrate layer and the second flexible glass substrate layer.

### Claim 7 (depends on 6)

The glass-polymer laminate structure of claim 6, wherein in-plane compressive stresses generated across a thickness of the first flexible glass substrate layer and a thickness of the second flexible glass substrate layer are compensated by tensile stresses in the polymer layer.

### Claim 8 (depends on 6)

The glass-polymer laminate structure of claim 6, wherein the polymer layer extends beyond an outer edge of at least one of the first and the second flexible glass substrates to form an edge protection feature.

### Claim 9 (depends on 1)

The glass-polymer laminate structure of claim 1, wherein the flexible glass substrate and the laminate layer are heated to a lamination temperature.

### Claim 10 (depends on 9)

The glass-polymer laminate structure of claim 9, wherein the lamination temperature is from about 80° C. to about 160° C.

### Claim 11 (depends on 1)

The glass-polymer laminate structure of claim 1, wherein the glass substrate is formed by a fusion process.

### Claim 12 (depends on 1)

The glass-polymer laminate structure of claim 1, wherein the polymer layer comprises at least one polymer selected from the group of polyethylene teraphthalate (PET), polyethylene naphthalate (PEN), ethylene tetrafluoroethylene (ETFE), thermopolymer polyolefin, polyesters, polycarbonate, polyvinylbuterate, polyvinyl chloride, polyethylene and substituted polyethylenes, polyhydroxybutyrates, polyhydroxyvinylbutyrates, polyetherimides, polyamides, polyethylenenaphalate, polyimides, polyethers, polysulphones, polyvinylacetylenes, transparent thermoplastics, transparent polybutadienes, polycyanoacrylates, cellulose-based polymers, polyacrylates and polymethacrylates, polyvinylalcohol, polysulphides, polyvinyl butyral, polymethyl methacrylate, polysiloxanes and combinations thereof.

### Claim 13 (depends on 12)

The glass-polymer laminate structure of claim 12, wherein the polymer layer comprises polymethyl methacrylate.

### Claim 14 (depends on 1)

The glass-polymer laminate structure of claim 1, wherein the polymer layer is a laminated or composite structure.

### Claim 15 (depends on 1)

The glass-polymer laminate structure of claim 1, wherein the glass-polymer laminate is transparent.

### Claim 16 (depends on 1)

The glass-polymer laminate structure of claim 1, wherein the glass polymer laminate is flexible.

### Claim 17 (depends on 1)

The glass-polymer laminate structure of claim 1, further comprising more than 3 glass or polymer layers.

### Claim 18 (depends on 1)

The glass-polymer laminate structure of claim 1, further comprising functional layers.

### Claim 19 (depends on 18)

The glass-polymer laminate structure of claim 18 wherein said functional layer is selected from the group of thin film transistors (TFTs), diodes, photodiodes, triodes, photovoltaic cells, photocouplers, transparent electrodes, color filters and electroconductive layers.