# US 10,953,591 B2 · Embossed microporous membrane wipes and methods of manufacture and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,953,591 B2
- Document ID: US10953591B2
- Status: Granted
- Kind: B2
- Application number: 14/662,355
- Filed: 2015-03-19
- Published: 2015-09-24
- Granted: 2021-03-23
- Earliest claimed: 2014-03-19
- Assignees: Celgard, LLC
- Applicants: Celgard, LLC; Ezek Technology, Inc.
- Inventors: Karl F. Humiston; Kristoffer K. Stokes; Victor J. Lin; Jui-Hung Huang
- Web page: https://patentgrep.com/patent/US10953591B2

## CPC

- B29C 55/00: Shaping by stretching, e.g. drawing through a die; Apparatus therefor (B29C61/08 takes precedence)
- A45D 34/04: Appliances specially adapted for applying liquid, e.g. using roller or ball
- A45D 2200/1027: Tissues, i.e. thin applicator sheets
- A45D 2200/1063: Removing cosmetic substances, e.g. make-up
- B29C 55/16: simultaneously
- B29L 2031/755: {Membranes, diaphragms}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- A45D: HAIRDRESSING OR SHAVING EQUIPMENT (wigs, toupees or the like A41G3/00, A41G5/00; hairdressers' chairs A47C1/04; hair cutting appliances, razors B26B); EQUIPMENT FOR COSMETICS OR COSMETIC TREATMENTS, e.g. FOR MANICURING OR PEDICURING
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

An embossed porous membrane wipe and/or a method of making and/or using such embossed microporous membrane wipe. The preferred embossed microporous membrane wipe includes a microporous membrane embossed alone or with a polypropylene nonwoven. The nonwoven may be a spunbond, meltblown, and/or electrospun nonwoven. The microporous membrane may include a biaxially oriented microporous membrane. The biaxially oriented microporous membrane may be made from one or more block copolymers of polyethylene and/or polypropylene. A method of using such an embossed microporous membrane, composite or laminate wipe for skin oil blotting is also provided.

## Claims

### Claim 1

An embossed microporous membrane wipe comprising:
a membrane with an average pore size of about 0.50 microns, a porosity in a range of 20-80%, or a transverse direction tensile strength of ≥175 kgf/cm2;
the membrane is made of a polymer selected from the group consisting of polyolefins, polyamides, polyesters, polyacetals, polysulfides, polyvinyl alcohols, co-polymers thereof, and combinations thereof and a dry-stretch process; and
the membrane has substantially round shaped pores, and a ratio of machine direction tensile strength to transverse direction tensile strength in a range of 0.5 to 5.0, and an embossed section, wherein the embossed section has a thickness of about 13 microns and an un-embossed section has a thickness of from 19 to 20 microns.

### Claim 2 (depends on 1)

The embossed microporous membrane wipe of claim 1, being adapted for skin oil blotting, and/or for removal of fingerprint or smudges from surfaces.

### Claim 3 (depends on 1)

The embossed microporous membrane wipe of claim 1, wherein the microporous membrane wipe is at least one of: a single ply film, a bi-layer film, or a multi-ply film.

### Claim 4 (depends on 1)

The embossed microporous membrane wipe of claim 1 having characteristics comprising a puncture strength of 166 g; a MD Tensile strength of 846 kgf/cm2; and a TD Tensile strength of 369 kgf/cm2.

### Claim 5 (depends on 1)

The embossed microporous membrane wipe of claim 1 including a pattern in the wipe through embossing.

### Claim 6 (depends on 1)

The embossed microporous membrane wipe of claim 1 wherein the embossed section is continuous or discontinuous.

### Claim 7 (depends on 1)

The embossed microporous membrane wipe of claim 1 wherein the membrane is at least one of:
a single or multilayer membrane, a composite or laminate,
the polymer being a semi-crystalline polymer, or
said substantially round shaped pores having an aspect ratio in a range of 0.75 to 1.25.

### Claim 8 (depends on 7)

The embossed microporous membrane wipe according to claim 7, with said membrane further having at least one of:
a transverse direction tensile strength of at least about 225 kgf/cm2,
a transverse direction shrinkage of:
less than about 6.0% at 90° C.;
less than about 15.0% at 120° C.

### Claim 9 (depends on 7)

The embossed microporous membrane wipe of claim 7, wherein said membrane is at least one of a blown film, a slot die film, a single layer precursor formed by at least one of single layer extrusion and multilayer extrusion, or a multilayer precursor formed by at least one of coextrusion and lamination.

### Claim 10 (depends on 1)

The embossed microporous membrane wipe of claim 1 wherein the dry-stretch process including the steps of:
extruding the polymer into at least a single layer nonporous precursor, and
biaxially stretching the nonporous precursor to make it microporous, the biaxial stretching including a machine direction stretching and a transverse direction stretching, the transverse direction stretching including a simultaneous controlled machine direction relax.

### Claim 11 (depends on 1)

The embossed microporous membrane wipe of claim 1 wherein said membrane has substantially round shaped pores, a JIS Gurley of less than about 100, and a hydro-head pressure greater than about 140 psi.

### Claim 12 (depends on 11)

The embossed microporous membrane wipe of claim 11 wherein a ratio of machine direction tensile strength to transverse direction tensile strength in the range of about 1.0 to 5.0, and the JIS Gurley of less than about 60.

### Claim 13 (depends on 1)

The embossed microporous membrane wipe of claim 1, further comprising a nonwoven laminated to said membrane, the nonwoven is selected from the group consisting of: a meltblown nonwoven material, and an electrospun nonwoven material.

### Claim 14 (depends on 13)

The embossed microporous membrane wipe according to claim 13, wherein the nonwoven is a polypropylene (PP) nonwoven.

### Claim 15 (depends on 13)

The embossed microporous membrane wipe according to claim 13, wherein laminating is adhesive or thermal lamination, embossing, calendering, or combinations thereof.

### Claim 16 (depends on 1)

A method of blotting oil from one's skin or face comprising the steps of:
providing an embossed microporous membrane wipe of claim 1; and
blotting oil from one's skin or face using said embossed microporous membrane wipe.

### Claim 17 (depends on 1)

A method of cleaning a surface comprising the steps of:
providing an embossed microporous membrane wipe of claim 1; and
wiping said surface with said embossed microporous membrane wipe.

### Claim 18 (depends on 17)

The method of claim 17 wherein said surface being selected from the group consisting of: eyeglasses; electronics; cell phones; displays; optical devices; camera lenses; microscope lenses; optics; and combinations thereof.

### Claim 19

A method of making an embossed microporous membrane wipe, an embossed microporous membrane wipe for skin oil blotting, or an embossed microporous membrane wipe for removal of fingerprint and/or smudges from surfaces comprising the steps of:
extruding, via a dry-stretch process, a polymer into a nonporous precursor, the precursor consisting of a polymer selected from the group consisting of polyolefins, polyamides, polyesters, polyacetals, polysulfides, polyvinyl alcohols, co-polymers thereof, and combinations thereof,
biaxially stretching the nonporous precursor to form a biaxially stretched membrane, the biaxial stretching including a machine direction stretching and a transverse direction stretching, the transverse direction stretching including a simultaneous controlled machine direction relax; and
embossing the biaxially stretched membrane, the membrane having an embossed section and a thickness of the embossed section of about 13 microns and of an un-embossed section of from 19 to 20 microns, an average pore size of about 0.50 microns, a porosity in a range of 20-80%, or a transverse direction tensile strength of ≥175 kgf/cm2; and
laminating a nonwoven to said membrane, wherein the nonwoven is selected from the group consisting of: a meltblown nonwoven material, and an electrospun nonwoven material.

### Claim 20 (depends on 19)

The method according to claim 19 wherein at least one of:
(1) wherein the polymer excludes any oils for subsequent removal to form pores or any pore-forming materials to facilitate pore formation,
(2) wherein the polymer being a semi-crystalline polymer,
(3) wherein the method comprises: annealing the nonporous precursor after extruding and before biaxially stretching, wherein annealing being conducted at a temperature in the range of Tm−80° C. to Tm−10° C.,
(4) wherein the biaxially stretching comprises: machine direction stretching, and thereafter transverse direction stretching including a simultaneous machine direction relax,
(5) wherein machine direction stretching being conducted either hot or cold or both,
(6) wherein cold machine direction stretching being conducted at a temperature <Tm−50° C. and/or hot machine direction stretching being conducted at a temperature <Tm−10° C.,
(7) wherein the total machine direction stretch being in the range of 50-500%, the total transverse direction stretch being in the range of 100-1200%, the machine direction relax from the transverse direction stretch being in the range of 5-80%, or combinations thereof, and
(8) wherein the method comprises providing a nonwoven on one side of said biaxially stretched membrane.