# US 10,953,568 B2 · Method for producing MDF boards with NFC/MFC

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,953,568 B2
- Document ID: US10953568B2
- Status: Granted
- Kind: B2
- Application number: 15/556,971
- Filed: 2015-03-09
- Published: 2018-06-21
- Granted: 2021-03-23
- Earliest claimed: 2015-03-09
- Assignees: Investigaciones Forestales Bioforest S.A.
- Applicants: Investigaciones Forestales Bioforest S.A.
- Inventors: Olli Joutsimo; Bruno Gorrini
- Web page: https://patentgrep.com/patent/US10953568B2

## CPC

- B27N 3/08: Moulding or pressing (presses in general B30B)
- B27N 3/04: from fibres
- B32B 5/02: characterised by structural features of a {fibrous or filamentary} layer {(layer formed of metallic wires B32B15/02; layer formed of natural mineral fibres B32B19/02; layer formed of wood fibres B32B21/02)}
- C09J 11/06: organic
- B27N 1/02: Mixing the material with binding agent (mixing in general B01F)
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

The invention relates to a method for the production of MDF boards, fibre and particle boards, based on cellulose fibres, comprising the following steps: obtaining wood chips; transporting them to a vaporizer silo where they are heated; transporting the wood chips to a digester where they continue to be heated and are conveyed via a supply outlet screw towards a shredder/refiner; adding a paraffinic emulsion to the chips; transporting them towards the shredder/refiner; injecting resin; carrying to a dryer; transporting towards a fibre silo; carrying the fibres to a step of forming, pre-pressing, pressing, measuring, classification, cooling, standing, formatting and packaging of the boards produced, wherein nanofibrillated cellulose (NFC) is added, together with microfibrillated cellulose (MFC), be it in the supply screw, or after the shredder/refiner, or after the dryer.

## Claims

### Claim 1

Method for producing MDF boards and fiber boards from cellulose fibers comprising the following steps:
a) obtaining wood chips and transporting them to a cleaning and classification process where they are washed;
b) transporting the cleaned chips to a steaming bin silo where they are heated;
c) transporting the chips from step (b) to a digester where they are further heated and conveyed via a supply outlet screw towards a shredder;
d) adding a wax emulsion or melted wax to said supply outlet screw towards the shredder or to a blowing line at an output of shredder towards a dryer;
e) transporting the chips from step (c) and wax emulsion to the shredder where they are mixed and the material is shredded to generate fibers from the shredder;
f) injecting resin in a blow line located at an input of the shredder or at the output of the shredder or at the output of the dryer;
g) carrying the mixture to the dryer, where water is evaporated and fibers from step (e) are dried;
h) transporting the dry fibers from step (g) to a fiber silo, which also receives fibers from different parts of the method where the fibers are stored and homogeneously mixed;
i) producing MDF boards or fiber boards leading the homogeneous fibers to a forming, pre-pressing, pressing, measuring, classification, cooling, sanding, and formatting and packaging step of the obtained board (MDF board or fiber board),
wherein nanofibrillated cellulose (NFC) is added together with microfibrillated cellulose (MFC) at the supply outlet screw of step c), or at the output of the shredder of step e), or at the output of the dryer of step g).

### Claim 2 (depends on 1)

Method according to claim 1, wherein the obtaining of chips is carried out by supplying wood to a debarker.

### Claim 3 (depends on 1)

Method according to claim 1, wherein the resin used can be urea-formaldehyde (UF) or melamine-urea-formaldehyde (MUF) resin.

### Claim 4 (depends on 3)

Method according to claim 3, wherein the resin used is urea formaldehyde resin.

### Claim 5 (depends on 1)

Method according to claim 1, wherein the amount of resin used ranges from 5 to 25% by weight of resin in a dry basis of wood fiber, and having a concentration of 45 to 70% by weight of resin, the rest being water.

### Claim 6 (depends on 4)

Method according to claim 4, wherein U/F molar ratios range from 0.4 to 1.4, solids content ranges from 40 to 65% by weight, and viscosity ranges from 100 to 500 cps.

### Claim 7 (depends on 3)

Method according to claim 3, wherein when the resin is a MUF resin, the melamine content ranges from 0.3% to 17% by weight of melamine.

### Claim 8 (depends on 1)

Method according to claim 1, wherein the NFC/MFC concentrations range from 0.5 to 50% by weight of nanocellulose/weight of dry resin.

### Claim 9 (depends on 8)

Method according to claim 8, wherein concentrations of NFC/MFC range from 1 to 30% by weight of nanocellulose/weight of dry resin.

### Claim 10 (depends on 1)

Method according to claim 1, wherein the NFC/MFC is added at the supply outlet screw of step (c).

### Claim 11 (depends on 1)

Method according to claim 1, wherein the NFC/MFC is added after the shredder of step (e).

### Claim 12 (depends on 1)

Method according to claim 1, wherein the NFC/MFC is added after the dryer of step (g).

### Claim 13 (depends on 1)

Method according to claim 1, wherein the wax emulsion or melted wax is injected to said supply outlet screw.

### Claim 14 (depends on 1)

Method according to claim 1, wherein the wax emulsion or melted wax is injected at the blowing line from the shredder to the dryer.

### Claim 15 (depends on 1)

Method according to claim 1, wherein the resin is injected at the input of the shredder.

### Claim 16 (depends on 1)

Method according to claim 1, wherein the resin is injected at the output of the shredder.

### Claim 17 (depends on 1)

Method according to claim 1, wherein the resin is injected at the output of the dryer.

### Claim 18 (depends on 1)

Method according to claim 1, wherein heating of chips of step (b) is performed at 3 bar, with saturated vapor.

### Claim 19 (depends on 1)

Method according to claim 1, wherein the digester in step (c) is a vertical tube wherein chips are further heated with saturated vapor at 7 to 9 bar, for a period of 2 to 7 minutes.

### Claim 20 (depends on 1)

Method according to claim 1, wherein the dryer in step (g) comprises one step, and the heat source used consists of hot gasses or hot air coming from the energy station through pipes where it is mixed with fresh air to control the temperature.

### Claim 21 (depends on 1)

Method according to claim 1, wherein the dryer in step (g) comprises two steps, and the heat source used consists of hot gasses or hot air coming from the energy station through pipes where it is mixed with fresh air to control the temperature.

### Claim 22 (depends on 1)

Method according to claim 1, wherein the forming step of step (i) is performed via blow-molding, generating a continuous mat.

### Claim 23 (depends on 1)

Method according to claim 1, wherein the forming step of step (i) is performed via mechanical formation, generating a continuous mat.

### Claim 24 (depends on 1)

Method according to claim 1, wherein at the pre-pressing step of step (i), the height of the mat is reduced.

### Claim 25 (depends on 1)

Method according to claim 1, wherein the pressing step of step (i) is performed in a multi-plate press.

### Claim 26 (depends on 1)

Method according to claim 1, wherein the pressing step of step (i) is performed in a continuous press.

### Claim 27 (depends on 1)

Method according to claim 1, wherein optionally a catalyst is injected in step (f) separately to the resin.

### Claim 28 (depends on 1)

Method according to claim 1, wherein optionally a catalyst is injected in step (f) together with the resin.

### Claim 29 (depends on 27)

Method according to claim 27, wherein the catalyst is selected from ammonium sulfate, ammonium chloride, or ammonium nitrate.

### Claim 30 (depends on 28)

Method according to claim 28, wherein the catalyst is selected from ammonium sulfate, ammonium chloride, or ammonium nitrate.

### Claim 31 (depends on 27)

Method according to claim 27, wherein the concentration of the catalyst range from 0.1 to 5% by dry weight to dry basis resin.

### Claim 32 (depends on 28)

Method according to claim 28, wherein the concentration of the catalyst range from 0.1 to 5% by dry weight to dry basis resin.

### Claim 33 (depends on 1)

Method according to claim 1, wherein optionally together with the NFC/MFC mixture, one or more filling agents are added.

### Claim 34 (depends on 33)

Method according to claim 33, wherein the filling agent is selected from the group consisting of: calcium carbonate, clays, plaster, kaolin, and alumina-silicates.

### Claim 35 (depends on 34)

Method according to claim 34, wherein the filling agent is calcium carbonate.

### Claim 36 (depends on 33)

Method according to claim 33, wherein the concentration of filling agent ranges from 1 to 100% by weight, being dosed in the range of 1 to 30% by weight to resin.