# US 10,952,932 B2 · Blank and method for producing a tooth replacement part

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,952,932 B2
- Document ID: US10952932B2
- Status: Granted
- Kind: B2
- Application number: 16/322,135
- Filed: 2017-08-09
- Published: 2019-10-31
- Granted: 2021-03-23
- Earliest claimed: 2016-08-09
- Assignees: DENTSPLY SIRONA Inc.
- Applicants: Sirona Dental Systems GmbH
- Inventors: Michael Bäurer
- Web page: https://patentgrep.com/patent/US10952932B2

## CPC

- A61K 6/818: comprising zirconium oxide
- A61C 5/77: Methods or devices for making crowns
- A61C 13/0022: {Blanks or green, unfinished dental restoration parts}
- A61C 13/083: Porcelain or ceramic teeth {(A61C13/081 takes precedence; preparations A61K6/80)}
- C04B 35/486: Fine ceramics
- C04B 35/645: Pressure sintering
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3244: Zirconium oxides, zirconates, hafnium oxides, hafnates, or oxide-forming salts thereof
- C04B 2235/3262: Manganese oxides, manganates, rhenium oxides or oxide-forming salts thereof, e.g. MnO
- C04B 2235/3275: Cobalt oxides, cobaltates or cobaltites or oxide forming salts thereof, e.g. bismuth cobaltate, zinc cobaltite
- C04B 2235/444: Halide containing anions, e.g. bromide, iodate, chlorite
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/6026: Computer aided shaping, e.g. rapid prototyping
- C04B 2235/612: Machining
- C04B 2235/6562: Heating rate
- C04B 2235/6565: Cooling rate
- C04B 2235/661: Multi-step sintering
- C04B 2235/77: Density
- C04B 2235/9661: Colour
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- A61C: DENTISTRY; APPARATUS OR METHODS FOR ORAL OR DENTAL HYGIENE (non-driven toothbrushes A46B; {tongue scrapers A61B17/24;} preparations for dentistry A61K6/00; preparations for cleaning the teeth or mouth A61K8/00, A61Q11/00)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The invention relates to a blank for producing a tooth replacement part using a CAD/CAM device, comprising a block of a sintered material. Said block of sintered material has already been presintered in a sintering furnace at an initial sintering temperature between 1000° C. and 1250° C.

## Claims

### Claim 1

A blank for producing a tooth replacement part using a CAD/CAM device, the blank comprising;
a presintered block that has been heat-treated in a sintering furnace at an initial sintering temperature between 1000° C. and 1250° C. in order to obtain a predefined hardness and a mechanical structure of the block so that fracturing of the produced tooth replacement part at a defined heating rate corresponding to the initial sintering temperature, does not occur during sintering of the tooth replacement part, wherein the block is pressed from a powder of ceramic particles with a zirconium dioxide (Y—ZrO2) weight fraction of at least 90% and a specific surface area between 11 m2/g and 17 m2/g, such that a sintering time of the tooth replacement part is reduced, wherein the powder includes at least one dye and/or at least one oxide or chloride of a dye, for coloring the block, the at least one dye being terbium for a yellow color, which has no change in valence with rapid cooling and thus does not undergo a change in color.

### Claim 2 (depends on 1)

The blank according to claim 1, wherein the initial sintering temperature is between 1050° C. and 1200° C.

### Claim 3 (depends on 1)

The blank according to claim 1, wherein the block is pressed with a pressing pressure between 130 and 250 MPa.

### Claim 4 (depends on 1)

The blank according to claim 1, wherein the specific surface area of the powder is between 12 and 14 m2/g.

### Claim 5 (depends on 1)

The blank according to claim 1, wherein the powder includes an yttrium oxide weight fraction between 2% and 4.5%.

### Claim 6 (depends on 1)

A method for producing a tooth replacement part from a blank according to claim 1, wherein the tooth replacement part is sintered to final density in a sintering furnace according to a defined temperature profile, wherein, in the volume of the tooth replacement part, the tooth replacement part includes a largest possible sphere having a diameter under a limit value of 6 mm, wherein the temperature profile has a defined heating rate between 150° C./minute and 350° C./minute in a heating phase and/or a defined cooling rate between 150° C./minute and 350° C./minute in a cooling phase.

### Claim 7 (depends on 6)

The method according to claim 6, wherein, in the volume of the tooth replacement part, the tooth replacement part includes a largest possible sphere having a diameter under a limit value of 3 mm, wherein the defined heating rate is between 200° C./minute and 350° C. minute.

### Claim 8 (depends on 1)

The blank according to claim 1, wherein the block is presintered ire order to obtain a predefined thermal conductivity of the block.

### Claim 9 (depends on 1)

The blank according to claim 1, wherein the defined heating rate is between 150° C./minute and 350° C./minute.

### Claim 10 (depends on 1)

The blank according to claim 1, wherein the defined heating rate is between 70° C./minute and 150° C. minute.