Method for impregnation of a part made of plastic material
AssigneeThe Swatch Group Research and Development Ltd
InventorNicolas Francois
Life of this patent
Estimating the term…
Abstract
A method for core impregnation of a finished part made of plastic material with an additive, including: dissolving the additive in a liquid medium to form a solution; placing the plastic part at ambient pressure in a pressure enclosure; hermetically sealing the chamber; impregnating the plastic part with the solution by a fluid at supercritical or near supercritical conditions in the enclosure at a pressure between 3 MPa and 6 MPa, at a temperature between 25° C. and 65° C. for a duration between 1 minute and 15 minutes; releasing the pressure inside the enclosure so that the liquid medium diffuses outside the plastic part and to trap the additive inside the plastic part.
Claims18
A method for core impregnation of a finished part made of plastic material with at least one additive, the method comprising:
- dissolving the at least one additive in a liquid medium to form a solution;
- placing a plastic part at ambient pressure in a pressure enclosure;
- hermetically sealing the chamber;
- impregnating the plastic part with the solution by carbon dioxide in the enclosure at a pressure between 3 MPa and 6 MPa, at a temperature between 40° C. and 65° C. for a duration between 1 minute and 10 minutes;
- releasing the pressure inside the enclosure so that the liquid medium diffuses outside the plastic part and to trap the at least one additive inside the plastic part,
- wherein the plastic part is a watch case, a watch wristband, a watch bezel, a watch crown, a watch dial, a watch push-button, a watch crystal, or a watch loop.
A method for core impregnation of a finished part made of plastic material with at least one additive, the method comprising:
- dissolving the at least one additive in a liquid medium to form a solution, wherein the at least one additive is a hyaluronic acid or ceramide;
- placing a plastic part at ambient pressure in a pressure enclosure;
- hermetically sealing the chamber;
- impregnating the plastic part with the solution by carbon dioxide in the enclosure at a pressure between 3 MPa and 6 MPa, at a temperature between 40° C. and 65° C. for a duration between 1 minute and 10 minutes;
- releasing the pressure inside the enclosure so that the liquid medium diffuses outside the plastic part and to trap the at least one additive inside the plastic part.