# US 10,876,190 B2 · Method of forming components from sheet material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,876,190 B2
- Document ID: US10876190B2
- Status: Granted
- Kind: B2
- Application number: 15/780,940
- Filed: 2016-12-05
- Published: 2018-10-25
- Granted: 2020-12-29
- Earliest claimed: 2015-12-04
- Assignees: Impression Technologies Limited
- Applicants: Impression Technologies Limited
- Inventors: Alistair Foster
- Web page: https://patentgrep.com/patent/US10876190B2

## CPC

- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/06: of magnesium or alloys based thereon
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

The present invention provides a method of forming a component (40) from an alloy sheet of material (30) having at least a Solvus temperature and a Solidus temperature of a precipitation hardening phase, the method comprising the steps of: heating the sheet (30) to above its Solvus temperature; initiating forming the heated sheet (30) between matched tools (32, 34) of a die press and forming by means of plastic deformation towards a final shape whilst allowing the average temperature of the sheet (30) to reduce at a first predetermined rate A; interrupting the forming of the sheet for a predetermined first interruption period P1 prior to achieving said final shape; and, during the interrupt holding the sheet of material with reduced or no deformation and allowing the average temperature of the sheet to reduce at a second predetermined rate B lower than or equal to the first predetermined rate in order to allow for a reduction in dislocations and completing the forming of the heated sheet into the final shape whilst allowing the sheet to cool at a third rate C greater than said second rate B.

## Claims

### Claim 1

A method of forming a component from an alloy sheet of material aluminum alloy or magnesium alloy having at least a Solvus temperature and a Solidus temperature of a precipitation hardening phase, the method comprising the steps of:
a. heating the alloy sheet to above its Solvus temperature;
b. initiating forming the heated alloy sheet between matched tools of a die press and forming by means of plastic deformation towards a final shape whilst allowing the average temperature of the alloy sheet to reduce at a first predetermined rate A;
c. interrupting the forming of the alloy sheet for a pre-determined first interruption period P1 prior to achieving said final shape; and, during the interrupt holding the alloy sheet with reduced or no deformation and allowing the average temperature of the alloy sheet to reduce at a second pre-determined rate B lower than or equal to the first predetermined rate in order to allow for a reduction in dislocations;
d. maintaining the interrupt step for a time such as to ensure the Dislocation Density is reduced whilst avoiding the precipitation of unwanted phases;
e. completing the forming of the heated alloy sheet into the final shape whilst allowing the alloy sheet to cool at a third rate C greater than said second pre-determined rate B.

### Claim 2 (depends on 1)

The method as claimed in claim 1 in which the alloy sheet is heated to within its Solution Heat Treatment temperature range during step(a).

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein said alloy sheet is formed to at least 50% of its final form during the initial forming of step (b).

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein said alloy sheet is formed to at least 90% of its final form during the initial forming of step (b).

### Claim 5 (depends on 1)

The method as claimed in claim 1 and including a second interruption period P2 after the first interrupt period P1 and before completion of the forming of step (e).

### Claim 6 (depends on 1)

The method as claimed in claim 1 and including multiple further interruption periods PX after the first interrupt period P1 and before completion of the forming of step (e).

### Claim 7 (depends on 1)

The method as claimed in claim 1 and wherein the method includes one or more interruption periods P1, P2, PX and wherein one or more of said one or more interruption periods includes a step of holding the matched tools in position.

### Claim 8 (depends on 1)

The method as claimed in claim 1 and wherein the method includes one or more interruption periods P1, P2, PX and wherein one or more of said one or more interruption periods includes a step of reversing the matched tools.

### Claim 9 (depends on 1)

The method as claimed in claim 1 and wherein the method includes one or more interruption periods P1, P2, PX and wherein one or more of said one or more interruption periods includes a step of holding and reversing the matched tools.

### Claim 10 (depends on 1)

The method as claimed in claim 1 and wherein the method includes one or more interruption periods P1, P2, PX and wherein the method includes the step of terminating the interruption period or periods prior to the precipitation of undesirable precipitates from a super saturated solid solution.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the temperature of the alloy sheet is maintained at a temperature of between 350° C. and 500° C. during the interrupt of step (c).

### Claim 12 (depends on 1)

The method according to claim 1, wherein the temperature of the alloy sheet is maintained at a temperature above 250° C. during the interrupt of step (c).

### Claim 13 (depends on 1)

The method according to claim 1 and including a step of maintaining the matched tools at a temperature of between −5° C. and +120° C. during the interrupt of step (c).

### Claim 14 (depends on 1)

The method as claimed in claim 1 and wherein the alloy sheet comprises an alloy from the 2xxx, 6xxx or 7xxx alloys.

### Claim 15 (depends on 1)

The method as claimed in claim 1 and wherein the alloy sheet is held during the interrupt of step (c) without deformation.

### Claim 16 (depends on 1)

The method as claimed in claim 1 and including a step of maintaining the metal sheet blank at a Solution Heat Treatment temperature until Solution Heat Treatment is complete.

### Claim 17 (depends on 1)

A method as claimed in claim 1 and including a step of holding a finished component between the matched tools after completion of step (e).