Method for obtaining calcium aluminates from non-saline aluminum slags
AssigneesArzyz, S.A. De C.V., Consejo Superior De Investigaciones Cientificas (Csic)
InventorsFelix Antonio Lopez Gomez, Francisco Jose Alguacil Priego, Jose Ramon Gonzalez Gracia, Mario Sergio Ramirez Zablah
Life of this patent
Estimating the term…
Abstract
The present invention relates to a method for obtaining calcium aluminates for metallurgical use from non-saline aluminum slags by means of reactive grinding and thermal treatment.
Claims6
A method for obtaining a mixture of the following calcium aluminates suitable for the manufacturing of steel:
- CaAl2O4(CA), CaAl4O7(CA2), Ca12Al14O33 (C12A7), Ca3AlO6 (C3A) and CaAl12O19 (CA6), where C═CaO and A=Al2O3, from a non-saline aluminum slag comprising the following steps:
- a) carrying out a reactive grinding of the non-saline aluminum slag from recovery by melting aluminum scrap metal or products of secondary melting of aluminum in the presence of calcium carbonate CaCO3, wherein the non-saline aluminum slag is generated from scrap metal and the reactive grinding of the non-saline aluminum slag with CaCO3 is carried out at a molar ratio of 1:3 Al2O3:CaO;
- b) thermally treating the product obtained in step a) at a temperature between 700° C. and 750° C. for one hour;
- and
- c) thermally treating the product obtained in step b) at a temperature between 1300° C. and 1400° C.
2 more elements