Laser welding member, and molded article
AssigneeMitsubishi Engineering-Plastics Corporation
InventorYasushi Yamanaka
Life of this patent
Estimating the term…
Abstract
A laser welding member that has a high laser transmittance at a welding region and exhibits an excellent laser welding processability, and a molded article obtained by laser welding using this laser welding member. The laser welding member is obtained by injection molding of a thermoplastic polyester resin material, wherein a region to be laser welded in the member is at a location separated by a distance of at least 15 mm from a gate of an injection molding mold and has at least 30% of a light transmittance of laser light with a wavelength of 940 nm.
Claims7
A method of producing a laser-welded molded article, the method comprising:
- laser welding a first laser welding member obtained by injection molding a thermoplastic polyester resin material, with a second member comprising a laser-absorptive resin material by irradiation with laser light from a side of the first laser welding member,
- wherein
- the thermoplastic polyester resin material of the first laser welding member comprises a polybutylene terephthalate resin, polystyrene and/or butadiene rubber-containing polystyrene, and a polycarbonate resin, and a content of the polybutylene terephthalate resin is from 30 to 90 mass %, a content of the polystyrene and/or butadiene rubber-containing polystyrene is from 1 to 50 mass %, and a content of the polycarbonate resin is from 1 to 50 mass %, based on 100 mass % for a total of the polybutylene terephthalate resin, the polystyrene and/or butadiene rubber-containing polystyrene, and the polycarbonate resin,
- the second member comprises a thermoplastic polyester resin composition comprising a carbon black or a laser light-absorbing dye,
- a region to be laser welded in the first member is at a location separated by a distance of at least 15 mm from a gate of an injection molding mold and has at least 50% of a light transmittance of laser light with a wavelength of 940 nm, and
- a crystallization temperature (Tc) of the region to be laser welded in the first member is not more than 188° C.
Dependencies are inferred from the claim text.