Process to prepare a heavy paraffin wax
AssigneeShell Oil Company
InventorsArend Hoek, Antonius Adrianus Maria Roovers, Kaushik Majumder
Life of this patent
Estimating the term…
Abstract
The present invention provides a paraffin wax having a congealing point according to ASTM D938 of at least 100° C. and a Saybolt colour according to ASTM D156 of at least 25 cm.
Claims16
A paraffin wax suitable for a hard wax application, the paraffin wax having a congealing point according to ASTM D938 of at least 108° C., a kinematic viscosity of at least 15 mm2/s at 120° C., and a Saybolt colour according to ASTM D156 of at least 25.
A paraffin wax suitable for a hard wax application, the paraffin wax having a congealing point according to ASTM D938 in the range of from 100 to 120° C., a kinematic viscosity of at least 15 mm2/s at 120° C., and a Saybolt colour according to ASTM D156 of at least 30.