# US 10,717,653 B2 · Graphene production by the thermal release of intrinsic carbon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,717,653 B2
- Document ID: US10717653B2
- Status: Granted
- Kind: B2
- Application number: 16/181,646
- Filed: 2018-11-06
- Published: 2019-05-09
- Granted: 2020-07-21
- Earliest claimed: 2017-11-08
- Assignees: Vaon, LLC
- Applicants: Vaon, LLC
- Inventors: Phillip C. Womble; Henry Steen; Melinda Whitfield Thomas; Jonathan C. Paschal; Quentin Lineberry; Richard C. Pape
- Web page: https://patentgrep.com/patent/US10717653B2

## CPC

- C01B 32/184: Preparation
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

The present invention generally relates to a process for manufacturing graphene coated surfaces using the intrinsic carbon within a metal.

## Claims

### Claim 1

A method of forming graphene, comprising:
(a) applying a vacuum to a furnace, the inside of the furnace comprising:
A. an oxygen scavenger; and,
B. a growth sample, the growth sample, comprising: a carbon-containing metal and a substrate, wherein the carbon-containing metal is in the form of a plurality of seeds that are in contact with the substrate;
(b) introducing a hydrogen-containing gas to the furnace;
(c) heating the inside of the furnace to a temperature and for a time sufficient to initiate graphene formation on the carbon-containing metal;
(d) cooling the furnace; and
(e) removing the seeds from the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the carbon-containing metal is selected from: Fe and Ni.

### Claim 3 (depends on 1)

The method of claim 1, wherein the carbon-containing metal is carbon steel.

### Claim 4 (depends on 1)

The method of claim 1, wherein the carbon-containing metal is 1095 steel.

### Claim 5 (depends on 1)

The method of claim 1, wherein the carbon-containing metal is grey steel.

### Claim 6 (depends on 1)

The method of claim 1, wherein the substrate is selected from: Cu, sapphire, and Ni on sapphire.

### Claim 7 (depends on 1)

The method of claim 1, wherein the substrate is Cu.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate is sapphire.

### Claim 9 (depends on 1)

The method of claim 1, wherein the substrate is Ni on sapphire.

### Claim 10 (depends on 1)

The method of claim 1, wherein the oxygen scavenger is Ti sponge.

### Claim 11 (depends on 1)

The method of claim 1, wherein the vacuum applied is ≤10 mTorr.

### Claim 12 (depends on 1)

The method of claim 1, wherein the vacuum applied is 2 mTorr.

### Claim 13 (depends on 1)

The method of claim 1, wherein the hydrogen-containing gas is introduced until the pressure of the furnace is from 20-150 mTorr.

### Claim 14 (depends on 1)

The method of claim 1, wherein the hydrogen-containing gas is a forming gas.

### Claim 15 (depends on 1)

The method of claim 1, wherein the hydrogen-containing gas is 95% Ar/5% H2.

### Claim 16 (depends on 1)

The method of claim 1, wherein the hydrogen-containing gas is 95% N2/5% H2.

### Claim 17 (depends on 1)

The method of claim 1, wherein the furnace is heated to a temperature of from 900-1100° C. for an hour.

### Claim 18 (depends on 1)

The method of claim 1, wherein the furnace is maintained at its highest temperature for 30-60 minutes.