The present invention provides a process for producing a friction material for a construction waste filler, including steps of: (S1) sorting a building material, removing fiber impurities, calcining, removing white garbage and metal impurities, and obtaining a first intermediate product; (S2) sifting and removing dust from the first intermediate product, obtaining an intermediate filler, cooling and then soaking after performing calcination on the intermediate filler, dehydrating, drying and obtaining a material to be mixed; (S3) evenly mixing the material to be mixed, graphite, molybdenum disulfide and other media materials, performing enhancement treatment, grinding and obtaining a building filler; and (S4) mixing composite fiber, phenolic resin, the building filler, friction material, pyrite, carbon black, alumina, and brass powder, stirring in a mixer for 20-40 min till all materials are fused, taking out a fused mixture, barreling, and obtaining the friction material for the construction waste filler.
A process for producing a friction material for a construction waste filler, comprising steps of:
Dependencies are inferred from the claim text.