US 10,647,835 B2Granted
Wear-resistant rubber compositions, systems, and methods
AssigneeWeir Slurry Group, Inc.
InventorsFrancisco A. Gozalo, Sanford W. Clark, Tham Meng, Timothy Lane
Life of this patent
Estimating the term…
Abstract
This disclosure relates to wear-resistant rubber compositions, such as those, for example, comprising at least one hydroxy-terminated polybutadiene, at least one natural rubber, at least one polymerization accelerant; at least one sulfur; and at least one polybutadiene, wherein the wear-resistant rubber composition may have an effective cross-linking density of at least about 30×10−5 moles/cm3.
Claims22
An extruded wear-resistant rubber composition comprising:
- at least one hydroxy-terminated polybutadiene;
- at least one natural rubber;
- at least one polymerization accelerant;
- at least one sulfur;
- at least one polybutadiene;
- at least one silica;
- and
- at least one silane,
- wherein the extruded wear-resistant rubber composition has an effective cross-linking density of at least about 30×10−5 moles/cm3.
6 more elements
An extruded wear-resistant rubber composition comprising:
- at least one hydroxy-terminated polybutadiene;
- at least one natural rubber;
- at least one polymerization accelerant;
- at least one sulfur;
- at least one polybutadiene;
- at least one silica;
- and
- at least one silane,
- wherein the extruded wear-resistant rubber composition has an effective cross-linking density of at least about 30×10−5 moles/cm3, and
- wherein the extruded wear-resistant rubber composition wears from about 10% to about 40% over a period of time, the period of time selected from the group consisting of about 1 week, about 3 weeks, about 7 weeks, about 14 weeks, about 21 weeks, and about 24 weeks.
7 more elements
A wear-resistant lifter bar assembly comprising:
- at least one rack for fixing the wear resistant lifter bar to a cylindrical wall of a rotating drum of a mill;
- and
- at least one wear body comprising an extruded wear resistant rubber composition, wherein the extruded wear resistant rubber composition comprises:
- at least one hydroxy-terminated polybutadiene;
- at least one natural rubber;
- at least one polymerization accelerant;
- at least one sulfur;
- at least one polybutadiene;
- at least one silica;
- and
- at least one silane,
- wherein the extruded wear-resistant rubber composition has an effective cross-linking density of at least about 30×10−5 moles/cm3.
9 more elements
Dependencies are inferred from the claim text.