Permanent magnet comprising a stack of N patterns
AssigneeCommissariat A L'energie Atomique Et Aux Energies Alternatives
InventorsBertrand Delaet, Sophie Giroud, Rachid Hida
Life of this patent
Estimating the term…
Abstract
A permanent magnet including, at least once per group of ten consecutive ferromagnetic layers, a growth layer directly interposed between a top antiferromagnetic layer of a previous pattern and a bottom antiferromagnetic layer of a following pattern. This growth layer is entirely realized in a nonmagnetic material chosen from the group made up of the following metals: Ta, Cu, Ru, V, Mo, Hf, Mg, NiCr and NiFeCr, or it is realized by a stack of several sublayers of nonmagnetic material disposed immediately on one another, at least one of these sublayers being entirely realized in a material chosen from the group. The thickness of the growth layer is greater than 0.5 nm.
Claims12
A permanent magnet comprising a stack of N patterns stacked one on top of another in a stack direction, wherein N is a whole number greater than or equal to two, wherein each pattern comprises:
- a bottom antiferromagnetic layer,
- a top antiferromagnetic layer, and
- a ferromagnetic layer situated between the bottom and top antiferromagnetic layers and whose direction of magnetization is frozen, by an exchange coupling, with the bottom or top antiferromagnetic layer of said pattern,
- the directions of magnetization of the ferromagnetic layers which are coupled by exchange coupling with the bottom or top antiferromagnetic layer of the same pattern are identical to each other,
- wherein:
- at least once per group of ten consecutive ferromagnetic layers whose directions of magnetization are frozen by exchange coupling, the stack comprises a growth layer interposed between the top antiferromagnetic layer of the previous pattern and the bottom antiferromagnetic layer of the following pattern in the stack direction and said growth layer is directly in contact with said two top and bottom antiferromagnetic layers between which the growth layer is interposed,
- the growth layer comprises a nonmagnetic material selected from the group consisting of Ta, Cu, Ru, V, Mo, Hf, Mg, NiCr and NiFeCr, or the growth layer comprises a stack of several sublayers, each comprising a nonmagnetic material, disposed immediately on one another in the stack direction, wherein at least one of the several sublayers is a metallic sublayer comprising a nonmagnetic material selected from the group consisting of Ta, Cu, Ru, V, Mo, Hf, Mg, NiCr and NiFeCr, and
- a thickness of the growth layer is greater than 0.5 nm.
A method of fabrication of a permanent magnet, the method comprising:
- a) forming a stack comprising N patterns stacked one upon the other in a stack direction, where N is a whole number greater than or equal to two, each pattern comprising:
- a bottom antiferromagnetic layer,
- a top antiferromagnetic layer, and
- a ferromagnetic layer situated between the bottom and top antiferromagnetic layers,
- b) heating the stack so as to achieve a temperature greater than a temperature of ordering of the material of the magnetic layers of the stack,
- c) when the temperature is greater than the temperature of the ordering, applying a first magnetic field to align the direction of magnetization of the ferromagnetic layers with a predetermined desired direction,
- d) cooling the stack in the presence of a second magnetic field less than the first magnetic field to cause an exchange coupling to appear between the ferromagnetic layer and the bottom or top antiferromagnetic layer of said pattern of the stack,
- wherein a) comprises forming, at least once per group of ten consecutive ferromagnetic layers whose directions of magnetization are frozen by exchange coupling, a growth layer interposed between the top antiferromagnetic layer of the previous pattern and the bottom antiferromagnetic layer of the following pattern in the stack direction,
- said growth layer is directly in contact with said two top and bottom antiferromagnetic layers between which the growth layer is interposed,
- said growth layer comprises a nonmagnetic material selected from the group consisting of Ta, Cu, Ru, Mo, Hf, Mg, NiCr and NiFeCr, or the growth layer comprises a stack of several sublayers of a nonmagnetic material disposed immediately on one another in the stack direction, wherein at least one of the several sublayers is a metallic sublayer comprising a nonmagnetic material selected from the group consisting of Ta, Cu, Ru, V, Mo, Hf, Mg, NiCr and NiFeCr, and
- a thickness of the growth layer is greater than 0.5 nm.