Nickel titanium alloys, methods of manufacture thereof and article comprising the same
AssigneeUniversity of Florida Research Foundation, Inc.
InventorsMichele Viola Manuel, Derek Hsen Dai Hsu
Life of this patent
Estimating the term…
Abstract
Disclosed herein is a shape memory alloy comprising 48 to 50 atomic percent nickel, 15 to 30 atomic percent hafnium, 1 to 5 atomic percent aluminum; with the remainder being titanium. Disclosed herein too is a method of manufacturing a shape memory alloy comprising mixing together to form an alloy nickel, hafnium, aluminum and titanium in amounts of 48 to 50 atomic percent nickel, 15 to 30 atomic percent hafnium, 1 to 5 atomic percent aluminum; with the remainder being titanium; solution treating the alloy at a temperature of 700 to 1300° C. for 50 to 200 hours; and aging the alloy at a temperature of 400 to 800° C. for a time period of 50 to 200 hours to form a shape memory alloy.
Claims6
A shape memory alloy comprising nickel (Ni), hafnium (Hf), aluminum (Al), and titanium, where the shape memory alloy has the formula Ni50Ti(30-x)Hf20Alx, where x has a value of 2 to 5, where the alloy displays a compressive strength of 900 to 1200 MPa at a compressive strain of 1.5 to 5%.
Dependencies are inferred from the claim text.