A producing method of a lithium-containing garnet crystal body which has a chemical composition represented by Li7-x-yLa3Zr2-x-yTaxNbyO12 wherein 0≤x≤0.8, 0.2≤y≤1, and 0.2≤x+y≤1, a relative density of 99% or greater, belongs to a cubic system, and has a garnet-related structure,
- wherein lithium ion conductivity of the lithium-containing garnet crystal body is equal to or greater than 1.0×10−3 S/cm, the method comprising:
- forming a melted portion at which single crystal is grown, by melting at least a portion of a raw material having a chemical composition represented by Li(7-x-y)zLa3Zr2-x-yTaxNbyO12 (0≤x≤0.8, 0.2≤y≤1, 0.2≤x+y≤1, and 1<z≤2);
- and
- moving the melted portion at a movement rate of 8 mm/h or faster to grow single crystal.