Horizontally wound coil of metallurgically heat treated metal tubing in a multi-layered configuration
AssigneeInductotherm Group Australia Pty Ltd.
InventorChristopher Gordon Stone
Life of this patent
Estimating the term…
Abstract
A horizontally wound continuous coil of metallurgically heat treated metal tubing is alternatively formed in a multi-layered configuration using a sequential four-layer or two-layer pattern of winding layer groups. The method of sequential four-layer or two-layer patterning of winding groups support formation of jumbo horizontally wound coils of continuous annealed copper tubing for use by end users of annealed copper tubing.
Claims3
A method of forming a horizontally wound coil of a lay stack of a heat treated metal tubing formed without a mandrel and from a linear feed of the heat treated metal tubing having an outer diameter, the lay stack having an outer lay stack radius and an inner lay stack radius, and a radial pitch distance equal to a distance between an interior centers of an adjacent turns of the heat treated metal tubing in a layer of the lay stack;
- characterized by:
- forming a repeating two-layer group of Layer 1 and Layer 2 of the heat treated metal tubing by:
- forming a Layer 1 outer turn of the heat treated metal tubing, the Layer 1 outer turn having the outer lay stack radius over a Layer 1 300 degrees rotation and a Layer 1 inner turn transition indexing radius equal to the outer lay stack radius minus the radial pitch distance over a Layer 1 60 degrees rotation;
- sequentially forming a plurality of Layer 1 inner turns where a Layer 1 inner turn radius of each successively inner one of the plurality of Layer 1 inner turns is decremented by the radial pitch distance from a previous Layer 1 inner turn radius of a previous inner one of the plurality of Layer 1 inner turns until a final Layer 1 inner turn radius of a Layer 1 final one of the plurality of Layer 1 inner turns is equal to the inner lay stack radius minus the radial pitch distance, each one of the plurality of Layer 1 inner turns having a Layer 1 inner turn radius over the Layer 1 300 degrees rotation and the Layer 1 inner turn transition indexing radius over the Layer 1 60 degrees rotation;
- indexing the heat treated metal tubing to the inner lay stack radius and forming a Layer 1 to Layer 2 transition turn of the heat treated metal tubing, the Layer 1 to Layer 2 transition turn having the inner lay stack radius over a Layer 1 to Layer 2 transition turn 300 degrees rotation and a Layer 1 to Layer 2 transition indexing over a Layer 1 to Layer 2 transition turn 60 degrees rotation;
- indexing the heat treated metal tubing to a sum of the inner lay stack radius and half of the radial pitch distance and forming a first Layer 2 inner turn radius equal to the sum of the inner lay stack radius and half of the radial pitch distance over a Layer 2 300 degrees rotation and indexing to a second Layer 2 turn transition over a Layer 2 60 degrees rotation to a second Layer 2 inner turn radius equal to the first Layer 2 inner turn radius incremented by the radial pitch distance;
- sequentially forming a plurality of Layer 2 outer turns where a Layer 2 outer turn radius of each successively outer one of the plurality of Layer 2 outer turns is incremented by the radial pitch distance from a previous Layer 2 outer turn radius of a previous outer one of the plurality of Layer 2 outer turns until the outer turn radius of a final one of the plurality of Layer 2 outer turns is equal to the outer lay stack radius minus half of the radial pitch distance, each one of the plurality of Layer 2 outer turns having the outer turn radius over the Layer 2 300 degrees rotation and the Layer 2 turn transition indexing over the Layer 2 60 degrees rotation;
- and
- forming a Layer 2 transition turn to the repeating two-layer group of Layer 1 and Layer 2 with a 360 degrees rotation of the heat treated metal tubing at the outer lay stack radius.
A method of forming a horizontally wound coil of a lay stack of a heat treated metal tubing formed without a mandrel and from a linear feed of the heat treated metal tubing having an outer diameter, the lay stack having an outer lay stack radius and an inner lay stack radius, and a radial pitch distance equal to a distance between an interior centers of an adjacent turns of the heat treated metal tubing in a layer of the lay stack;
- characterized by:
- forming a repeating four-layer group of Layer 1, Layer 2, Layer 3 and Layer 4 of the heat treated metal tubing by:
- forming a Layer 1 outer turn of the heat treated metal tubing, the Layer 1 outer turn having the outer lay stack radius over a Layer 1 300 degrees rotation and a Layer 1 inner turn transition indexing of the radial pitch distance over a Layer 1 60 degrees rotation;
- sequentially forming a plurality of Layer 1 inner turns where a Layer 1 inner turn radius of each successively inner one of the plurality of Layer 1 inner turns is decremented by the radial pitch distance from a previous Layer 1 inner turn radius of a previous inner one of the plurality of Layer 1 inner turns until a final Layer 1 inner turn radius of a Layer 1 final one of the plurality of Layer 1 inner turns is equal to the inner lay stack radius minus the radial pitch distance, each one of the plurality of Layer 1 inner turns having a Layer 1 inner turn radius over the Layer 1 300 degrees rotation and the Layer 1 inner turn transition indexing of the radial pitch distance over the Layer 1 60 degrees rotation;
- forming a Layer 1 to Layer 2 transition turn of the heat treated metal tubing, the Layer 1 to Layer 2 transition turn having the inner lay stack radius over a Layer 1 to Layer 2 transition turn 300 degrees rotation and a Layer 1 to Layer 2 transition indexing over a Layer 1 to Layer 2 transition turn 60 degrees rotation;
- sequentially forming a plurality of Layer 2 outer turns where a Layer 2 outer turn radius of each successively outer one of the plurality of Layer 2 outer turns is incremented by the radial pitch distance from a previous Layer 2 outer turn radius of a previous outer one of the plurality of Layer 2 outer turns until a final Layer 2 outer turn radius of a Layer 2 final one of the plurality of Layer 2 outer turns is equal to the outer lay stack radius, each one of the plurality of Layer 2 outer turns having a Layer 2 outer turn radius over a Layer 2 300 degrees rotation and a Layer 2 outer layer turn transition indexing of the radial pitch distance over a Layer 2 60 degrees rotation;
- forming a Layer 2 to Layer 3 transition turn of the heat treated metal tubing, the Layer 2 to Layer 3 transition turn having a Layer 2 to Layer 3 transition turn outer lay stack radius over a Layer 2 to Layer 3 transition turn 300 degrees rotation a Layer 2 to Layer 3 transition indexing over a 60 degree rotation;
- sequentially forming a plurality of Layer 3 inner turns where a Layer 3 inner turn radius of each successively inner one of the plurality of Layer 3 inner turns is decremented by the radial pitch distance from a previous Layer 3 inner turn radius of a previous inner one of the plurality of Layer 3 inner turns until a final Layer 3 inner turn radius of a Layer 3 final one of the plurality of Layer 3 inner turns is equal to the inner lay stack radius minus the radial pitch distance, each one of the plurality of Layer 3 inner turns having a Layer 3 inner turn radius over a Layer 3 300 degrees rotation and the Layer 3 inner layer turn transition indexing of the radial pitch distance over the Layer 3 60 degrees rotation;
- forming a Layer 3 to Layer 4 transition turn of the heat treated metal tubing, the Layer 3 to Layer 4 transition turn having a Layer 3 to Layer 4 transition turn inner lay stack radius over a Layer 3 to Layer 4 transition turn 300 degrees rotation and a Layer 3 to Layer 4 transition indexing over a Layer 3 to Layer 4 transition turn 60 degrees rotation;
- sequentially forming a plurality of Layer 4 outer turns where a Layer 4 outer turn radius of each successively outer one of the plurality of Layer 4 outer turns is incremented by the radial pitch distance from a previous Layer 4 outer turn radius of a previous outer one of the plurality of Layer 4 outer turns until a final Layer 4 outer turn radius of a Layer 4 final one of the plurality of Layer 4 outer turns is equal to the outer lay stack radius, each one of the plurality of Layer 4 outer turns having a Layer 4 outer turn radius over a Layer 4 300 degrees rotation and a Layer 4 outer layer turn transition indexing of the radial pitch distance over a Layer 4 60 degrees rotation;
- and
- forming a Layer 4 transition to the repeating four-layer group of Layer 1, Layer 2, Layer 3 and Layer 4 of the heat treated metal tubing with a 360 degrees rotation of the heat treated metal tubing at the outer lay stack radius.
A method of forming a horizontally wound coil of a lay stack of a heat treated metal tubing formed without a mandrel and from a linear feed of the heat treated metal tubing having an outer diameter, the lay stack having an outer lay stack radius and an inner lay stack radius, and a radial pitch distance equal to a distance between an interior centers of an adjacent turns of the heat treated metal tubing in a layer of the lay stack;
- characterized by:
- forming a repeating four-layer group of Layer 1, Layer 2, Layer 3 and Layer 4 of the heat treated metal tubing by:
- forming a Layer 1 outer turn of the heat treated metal tubing, the Layer 1 outer turn having the outer lay stack radius over a Layer 1 300 degrees rotation and a Layer 1 inner turn transition indexing of the radial pitch distance over a Layer 1 60 degrees rotation;
- sequentially forming a plurality of Layer 1 inner turns where a Layer 1 inner turn radius of each successively inner one of the plurality of Layer 1 inner turns is decremented by the radial pitch distance from a previous Layer 1 inner turn radius of a previous inner one of the plurality of Layer 1 inner turns until a final Layer 1 inner turn radius of a Layer 1 final one of the plurality of Layer 1 inner turns is equal to the inner lay stack radius minus the radial pitch distance, each one of the plurality of Layer 1 inner turns having a Layer 1 inner turn radius over the Layer 1 300 degrees rotation and the Layer 1 turn transition indexing of the radial pitch distance over the Layer 1 60 degrees rotation;
- forming a Layer 1 to Layer 2 transition turn of the heat treated metal tubing having a Layer 1 to Layer 2 transition turn inner lay stack radius over a Layer 1 to Layer 2 transition turn 300 degrees rotation and a Layer 1 to Layer 2 transition indexing of the radial pitch distance over a Layer 1 to Layer 2 transition turn 60 degrees rotation;
- indexing the Layer 1 to Layer 2 transition turn over 60 degrees rotation to a first Layer 2 inner turn radius equal to a sum of the inner lay stack radius and a half of the radial pitch distance;
- forming the first Layer 2 turn of the heat treated metal tubing having the first Layer 2 inner turn radius equal to the sum of the inner lay stack radius and the half of the radial pitch distance over a Layer 2 300 degrees rotation and indexing a first Layer 2 turn transition over a Layer 2 60 degrees rotation to a first Layer 2 outer turn of a plurality of Layer 2 outer turns with an inner turn radius equal to the first Layer 2 inner turn radius incremented by the radial pitch distance;
- sequentially forming the plurality of Layer 2 outer turns where a Layer 2 outer turn radius of each successively outer one of the plurality of Layer 2 outer turns is incremented by the radial pitch distance from the outer turn radius of a previous outer one of the plurality of Layer 2 outer turns until a final outer turn radius of a final one of the plurality of Layer 2 outer turns is equal to the outer lay stack radius minus the radial pitch distance, each one of the plurality of Layer 2 outer turns having an outer turn radius over a Layer 2 300 degrees rotation and a Layer 2 outer layer turn transition indexing of the radial pitch distance over a Layer 2 60 degrees rotation;
- forming a Layer 2 to Layer 3 transition turn of the heat treated metal tubing having a Layer 2 to Layer 3 transition turn outer lay stack radius over a Layer 2 to Layer 3 transition turn 300 degrees rotation and a Layer 2 to Layer 3 transition indexing over a Layer 2 to Layer 3 transition turn 60 degree rotation;
- sequentially forming a plurality of Layer 3 inner turns where a Layer 3 inner turn radius of each successively inner one of the plurality of Layer 3 inner turns is decremented by the radial pitch distance from a previous Layer 3 inner turn radius of a previous inner one of the plurality of Layer 3 inner turns until a final Layer 3 inner turn radius of a Layer 3 final one of the plurality of Layer 3 inner turns is equal to the inner lay stack radius minus the radial pitch distance, each one of the plurality of Layer 3 inner turns having a Layer 3 inner turn radius over a Layer 3 300 degrees rotation and the Layer 3 inner layer turn transition indexing of the radial pitch distance over the Layer 3 60 degrees rotation;
- forming a Layer 3 to Layer 4 transition turn of the heat treated metal tubing having a Layer 3 to Layer 4 transition inner lay stack radius minus half of the radial pitch distance over a Layer 3 to Layer 4 transition turn 300 degrees rotation and a Layer 3 to Layer 4 transition indexing over a Layer 3 to Layer 4 transition turn 60 degrees rotation;
- sequentially forming a plurality of Layer 4 outer turns where a Layer 4 outer turn radius of each successively outer one of the plurality of Layer 4 outer turns is incremented by the radial pitch distance from a previous Layer 4 outer turn radius of a previous outer one of the plurality of Layer 4 outer turns until a final Layer 4 outer turn radius of a Layer 4 final one of the plurality of Layer 4 outer turns is equal to the outer lay stack radius minus half of the radial pitch distance, each one of the plurality of Layer 4 outer turns having a Layer 4 outer turn radius over a Layer 4 300 degrees rotation and a Layer 4 outer layer turn transition indexing over the a Layer 4 60 degrees rotation;
- and
- forming a Layer 4 transition to the repeating four-layer group of Layer 1, Layer 2, Layer 3 and Layer 4 with a 360 degrees rotation of the heat treated metal tubing at the outer lay stack radius.
Dependencies are inferred from the claim text.