# US 10,526,538 B2 · Methods, process and fabrication technology for high-efficiency low-cost crystalline silicon solar cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,526,538 B2
- Document ID: US10526538B2
- Status: Granted
- Kind: B2
- Application number: 14/549,261
- Filed: 2014-11-20
- Published: 2015-06-11
- Granted: 2020-01-07
- Earliest claimed: 2010-09-16
- Assignees: Specmat Limited
- Applicants: Maria Faur; Horia M. Faur
- Inventors: Maria Faur; Horia M. Faur; Mircea Faur
- Web page: https://patentgrep.com/patent/US10526538B2

## CPC

- C09K 13/08: containing a fluorine compound
- C23F 1/16: Acidic compositions (C23F1/42 takes precedence)
- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/129: {Passivating}
- H10F 77/211: {for photovoltaic cells}
- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 77/48: Back surface reflectors [BSR]
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02E 10/52: PV systems with concentrators
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a method, process, solar cell design, and fabrication technology fir high-efficiency, low-cost, crystalline silicon (Si) solar cells including but not restricted to solar grade single crystal Si (c-Si), multi-crystalline Si (mc-Si), poly-Si, and micro-Si solar cells and solar modules. The RTWCG solar cell fabrication technology creates a RTWCG SiOx thin film antireflection coating (ARC) with a graded index of refraction and a selective emitter (SE). The resulting top surface of the SiOx oxide can be textured (TO) concomitant with the growth process or through an additional mild wet chemical step.

## Claims

### Claim 1

A composition for growing an oxide layer on a substrate, the composition comprising: a fluoride source selected from HF; an inorganic oxidant containing iodine, or a combination of both iodine and silver, to promote an oxidation reaction at a surface of the substrate and thereby facilitate growing of the oxide layer on the substrate based at least in part on consumed substrate resulting from the etching of the substrate; and a non-invasive additive to control a balance between a first rate of the etching of the substrate and a second rate of the growing of the oxide layer, wherein the composition is substantially free of silicon, wherein the inorganic oxidant contains at least one iodine compound selected from HIO3, I2O4, I2O5 and I2O9 at a concentration of between about 0.026 weight percent and about 0.19 weight percent, and wherein the pH of the composition is sufficient to wet etch a substrate and achieve oxide layer growth due to the presence of HF at a concentration of between 10 weight percent and 50 weight percent.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the composition is substantially free of organic components.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the inorganic oxidation system is selected from HIO3.

### Claim 4 (depends on 3)

The composition of claim 3, wherein the non-invasive additive is HCl.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the non-invasive additive is selected from NH4F, HF, HCl, H2O, HNO3 and H2O2.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the non-invasive additive is HCl.

### Claim 7 (depends on 1)

The composition of claim 1, further comprising water.

### Claim 8 (depends on 1)

The composition of claim 1, further comprising an acid.

### Claim 9 (depends on 8)

The composition of claim 8, wherein the acid is selected from H2SiF6, HCl, HF, HNO3, and H2SO4.

### Claim 10

A composition for room temperature wet chemical growth of an oxide-based layer on a substrate, the composition consisting essentially of HF, HCl, and an iodine-containing inorganic oxidation system and water, wherein the composition is substantially free of silicon and the iodine-containing inorganic oxidation system is selected from HIO3, I2O4, I2O5 and I2O9 at a concentration of between about 0.026 weight percent and about 0.19 weight percent, and wherein the pH of the composition is sufficient to wet etch a substrate and achieve oxide layer growth due to the presence of HF at a concentration of between 10 weight percent and 50 weight percent.

### Claim 11 (depends on 10)

The composition of claim 10, wherein the composition is substantially free of organic components.

### Claim 12 (depends on 10)

The composition of claim 10, wherein the inorganic oxidation system is selected from HIO3.

### Claim 13 (depends on 10)

The composition of claim 10, wherein the substrate comprises one or more of silicon, germanium, and gallium arsenide, and wherein the HF facilitates etching of the one or more of silicon, germanium, and gallium arsenide.

### Claim 14 (depends on 10)

The composition of claim 10, wherein the substrate comprises single crystal silicon or polycrystalline silicon, and wherein the HF facilitates etching of the single crystal silicon or the polycrystalline silicon.

### Claim 15

A composition to facilitate fabrication of a solar cell on a substrate by substantially simultaneously accomplishing (i) wet chemical etching of the substrate and (ii) growing, at substantially room temperature, an oxide layer on the substrate, the oxide layer forming at least one of an antireflective coating for the solar cell, a layer in an anti-reflective coating stack for the solar cell, a passivation layer for the solar cell, and a mask for the fabrication of the solar cell, the oxide layer having:
a formulation SixOyXz, wherein X, when present, is selected from at least one of fluorine (F), carbon (C), hydrogen (H), iodine (I), vanadium (V), cobalt (Co), lead (Pb), silver (Ag) and nitrogen (N); and
a thickness of less than or equal to 500 nanometers,
the composition comprising:
a fluoride source selected from HF at a concentration of between 10 weight percent and 50 weight percent to facilitate the etching of the substrate;
an inorganic oxidant containing iodine, or a combination of both iodine and silver, to promote an oxidation reaction at a surface of the substrate and thereby facilitate the growing of the oxide layer on the substrate based at least in part on consumed substrate resulting from the etching of the substrate; and
a non-invasive inorganic additive to control a balance between a first rate of the etching of the substrate and a second rate of the growing of the oxide layer,
wherein the composition is substantially free of silicon, and wherein the inorganic oxidant contains at least one iodine compound selected from HIO3, I2O4, I2O5 and I2O9 at a concentration of between about 0.026 weight percent and about 0.19 weight percent.

### Claim 16 (depends on 15)

The composition of claim 15, wherein:
the substrate includes a diffused region constituting an emitter of the solar cell;
the composition facilitates fabrication by substantially simultaneously accomplishing (i) wet chemical etching of the diffused region of the substrate constituting the emitter of the solar cell and (ii) growing, at substantially room temperature, the oxide layer on the diffused region;
the fluoride source facilitates the etching of the diffused region of the substrate constituting the emitter of the solar cell;
the inorganic oxidant promotes the oxidation reaction at the surface of the diffused region and thereby facilitates growth of the oxide layer on the diffused region based at least in part on the consumed substrate resulting from the etching of the diffused region; and
the non-invasive inorganic additive controls the balance between the first rate of the etching of the diffused region and the second rate of the growing of the oxide layer.

### Claim 17

A composition for growing an oxide layer on a substrate, the composition comprising: a fluoride source; an inorganic oxidant, containing at least one source of iodine, or at least one source of iodine in combination with at least one source of silver, to promote an oxidation reaction at a surface of the substrate and thereby facilitate growing of the oxide layer on the substrate based at least in part on consumed substrate resulting from the etching of the substrate; and a non-invasive additive to control a balance between a first rate of the etching of the substrate and a second rate of the growing of the oxide layer, wherein the composition is substantially free of silicon, wherein the inorganic oxidant contains at least one source of iodine selected from HIO3, I2O4, I2O5 and I2O9 at a concentration of between about 0.026 weight percent and about 0.19 weight percent, and wherein the pH of the composition is sufficient to wet etch a substrate and achieve oxide layer growth due to the presence of HF at a concentration of between 10 weight percent and 50 weight percent.