Back to results
US 10,526,253 B2Granted
High temperature oxidation protection for composites
AssigneeGoodrich Corporation
InventorSteven A. Poteet
Life of this patent
Estimating the term…
Abstract
The present disclosure provides a method for coating a composite structure, comprising forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate; applying the first slurry on a surface of the composite structure to form a base layer; and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.
Claims11
A method for coating a composite structure, comprising:
- forming a first slurry by combining a first pre-slurry composition comprising a first phosphate glass composition, with a primary flow modifier, a secondary flow modifier, and a first carrier fluid, wherein the primary flow modifier comprises at least one of cellulose or calcium silicate, and wherein the secondary flow modifier comprises at least one of poly(vinyl alcohol) or a salt of poly(acrylic acid);
- applying the first slurry on a surface of the composite structure to form a base layer;
- and heating the composite structure to a temperature sufficient to adhere the base layer to the composite structure.