# US 10,501,363 B2 · Method for producing photo-structurable glass bodies by a redrawing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,501,363 B2
- Document ID: US10501363B2
- Status: Granted
- Kind: B2
- Application number: 15/158,223
- Filed: 2016-05-18
- Published: 2016-11-24
- Granted: 2019-12-10
- Earliest claimed: 2015-05-18
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Carsten Renz; Marten Walther; Lothar Niessner; Martin Feichtinger; Bianca Schreder; Junming Xue; Sean Qian
- Web page: https://patentgrep.com/patent/US10501363B2

## CPC

- C03C 3/093: containing zinc or zirconium
- C03B 23/047: by drawing ({C03B23/091} , C03B37/025 takes precedence)
- C03B 32/00: Thermal after-treatment of glass products not provided for in groups {C03B19/00} , C03B25/00 - C03B31/00 {or C03B37/00}, e.g. crystallisation, eliminating gas inclusions or other impurities; {Hot-pressing vitrified, non-porous, shaped glass products}
- C03C 3/085: containing an oxide of a divalent metal
- C03C 4/04: for photosensitive glass
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 23/002: {by ultraviolet light}
- C03B 5/193: using gas, e.g. bubblers
- C03B 19/02: by casting {molten glass, e.g. injection moulding}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method for production of a photo-structurable glass element is provided. The method includes the steps of: fixing a blank of photo-structurable glass at a first end; heating of a deformation zone of the blank; and drawing the blank. The glass includes Si4+, a crystal-agonist, a crystal-antagonist, and a pair of nucleating agents. The crystal-agonist is selected from the group consisting of Na+, K+, Li+, and any combinations thereof. The crystal-antagonist is selected from the group consisting of Al3+, B3+, Zn2+, Sr2+, Sb3+, and any combinations thereof. The pair of nucleating agents include cerium and an agent selected from the group consisting of silver, gold, copper, and any combinations thereof. The crystal-agonist has a molar proportion cat.-% in relation to a molar proportion of Si4+ that is at least 0.3 and at most 0.85.

## Claims

### Claim 1

A method for production of a photo-structurable glass element, comprising the steps of:
a. fixing a blank of photo-structurable glass at a first end;
b. heating of a deformation zone of the blank;
c. drawing the blank; and
d. subsequent to either step b. or step c., a sensitization step comprising cooling the blank from a first temperature to a second temperature with an average cooling rate K of at most 200° C./h, wherein the first temperature is at least above a glass transition temperature of the photo-structurable glass and the second temperature is at least 150° C. below the first temperature,
wherein the glass comprises Si4+, a crystal-agonist, a crystal-antagonist, and a pair of nucleating agents,
wherein the crystal-agonist is selected from the group consisting of Na+, K+, Li+, and any combinations thereof,
wherein the crystal-antagonist is selected from the group consisting of Al3+, B3+, Zn2+, Sn2+, Sb3+, and any combinations thereof,
wherein the pair of nucleating agents comprises cerium and an agent selected from the group consisting of silver, gold, copper, and any combinations thereof, and
wherein the crystal-agonist has a molar proportion cat.-% in relation to a molar proportion of Si4+ that is at least 0.3 and at most 0.85,
wherein lithium with regard to the molar proportion exceeds the proportions of the components sodium and potassium in the glass, and
wherein the glass has a transmittance value of the at least 0.2% at a wavelength of 260 nm and a sample thickness of 1 mm after the sensitization step.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the average cooling rate K is of from 10° C./h to 200° C./h.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the step of subjecting the blank to the sensitization step is subsequent to the heating step.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the step of subjecting the blank to the sensitization step is subsequent to the drawing step.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the photo-structurable glass comprises the following components in cat.-%
Si4+
45 to 65
Crystal-agonists
30 to 45
Crystal-antagonists
3.5 to 9.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the photo-structurable glass has the following components in cat.-%
Si4+
45 to 65
Crystal-agonists
Li+
25 to 40
K+
0 to 8
Na+
0 to 8
Crystal-antagonists
B3+
0 to 5
Al3+
0 to 10
Zn2+
0 to 4
Sb3+
0 to 0.4
Nucleating agents
Ce3+/Ce4+
>0 to 0.3
Ag+
>0 to 0.5.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the photo-structurable glass comprises between 0.02 and 0.2 cat.-% Sb3+.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the photo-structurable glass comprises anions and cations and comprises a molar proportion of O2− with regard to the anions of at least 99%.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the glass has a transmittance value of at most 5% at a wavelength of 260 nm and a sample thickness of 1 mm.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the glass has a transmittance value of at least 8% and at most 30% at a wavelength of 280 nm and a sample thickness of 1 mm.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the standard deviation of the transmittance of the glass which constitutes the glass element at a wavelength of 260 nm and/or 280 nm is at most 15% of the respective mean value of transmittance, wherein mean value and standard deviation are determined from at most 100 independent measured values.