# US 10,483,521 B2 · Sealed battery and manufacturing method of sealed battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,483,521 B2
- Document ID: US10483521B2
- Status: Granted
- Kind: B2
- Application number: 16/106,837
- Filed: 2018-08-21
- Published: 2019-03-07
- Granted: 2019-11-19
- Earliest claimed: 2017-09-07
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Tomohiro Ono; Yuta Nemoto
- Web page: https://patentgrep.com/patent/US10483521B2

## CPC

- H01M 50/578: in response to pressure
- H01M 4/0419: {involving spraying}
- H01M 50/24: adapted for protecting batteries from their environment, e.g. from corrosion (thermal insulation H01M10/658)
- H01M 50/3425: {in the form of rupturable membranes or weakened parts, e.g. pierced with the aid of a sharp member}
- H01M 50/531: Electrode connections inside a battery casing
- H01M 50/188: the sealing members being arranged between the lid and terminal
- H01M 2200/00: Safety devices for primary or secondary batteries
- H01M 2200/10: Temperature sensitive devices
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A sealed battery includes a battery outer case, a collector terminal, an outwardly exposed terminal, and a current shut-off mechanism configured to cut off a conductive path from the collector terminal to the outwardly exposed terminal when the internal pressure of the battery outer case exceeds a predetermined pressure. The current shut-off mechanism includes a connection plate with a vent hole, and a shut-off valve including a reversing portion. A joint region in the connection plate is in contact with a surface, of the reversing portion, that faces the inner side of the battery outer case. A thermal-spray joint portion configured to cover a border between the joint region and the reversing portion is provided, such that the shut-off valve is joined to the connection plate via the thermal-spray joint portion.

## Claims

### Claim 1

A sealed battery comprising:
a battery outer case in which an electrode body is accommodated;
a collector terminal electrically connected to the electrode body inside the battery outer case;
an outwardly exposed terminal electrically connected to the collector terminal inside the battery outer case and partially exposed outside the battery outer case; and
a current shut-off mechanism placed on a conductive path from the collector terminal to the outwardly exposed terminal and configured to cut off the conductive path when an internal pressure of the battery outer case exceeds a predetermined pressure, wherein:
the current shut-off mechanism includes a connection plate as a plate-shaped conductive member provided in one end of the collector terminal, the connection plate with a vent hole provided in a central part of the connection plate, and a shut-off valve including a reversing portion electrically connected to the outwardly exposed terminal;
a joint region is in a peripheral portion in the connection plate, the peripheral portion defining the vent hole of the connection plate;
the joint region is in contact with a surface of the reversing portion, the surface facing an inner side of the battery outer case;
a thermal-spray joint portion is provided so as to cover a border between the joint region and the reversing portion; and
the shut-off valve is joined to the connection plate via the thermal-spray joint portion.

### Claim 2 (depends on 1)

The sealed battery according to claim 1, wherein the reversing portion includes a dome-shaped concave portion that is concaved toward the inner side of the battery outer case.

### Claim 3 (depends on 1)

The sealed battery according to claim 1, wherein the joint region is configured such that a thickness of the connection plate is thinner in a tapered shape toward the vent hole.

### Claim 4 (depends on 3)

The sealed battery according to claim 3, wherein a tip end of the connection plate in the joint region defines the vent hole, and an angle of the tip end is between 20° and 40°.

### Claim 5 (depends on 1)

The sealed battery according to claim 1, wherein the thermal-spray joint portion is made of the same metallic, material as the connection plate and the shut-off valve.

### Claim 6 (depends on 5)

The sealed battery according to claim 5, wherein the thermal-spray joint portion is made of aluminum or aluminum alloy.

### Claim 7 (depends on 1)

The sealed battery according to claim 1, wherein a thickness of the thermal-spray joint portion is between 0.1 mm and 1.0 mm.

### Claim 8 (depends on 1)

The sealed battery according to claim 1, wherein the thermal-spray joint portion is an annular shape so as to cover a whole circumference of the peripheral portion.

### Claim 9 (depends on 1)

The sealed battery according to claim 1, wherein the joint region is perpendicular to the surface.

### Claim 10

A manufacturing method of a sealed battery, the manufacturing method comprising:
bringing a joint region formed in a peripheral portion defining a vent hole of a connection plate of the sealed battery into contact with a surface of a reversing portion of a shut-off valve of the sealed battery, the surface facing an inner side of a battery outer case in which an electrode body is accommodated; and
forming a thermal-spray joint portion such that a metallic material is sprayed so as to cover a border between the joint region and the reversing portion, wherein:
the sealed battery includes:
a collector terminal electrically connected to the electrode body inside the battery outer case;
an outwardly exposed terminal electrically connected to the collector terminal inside the battery outer case and partially exposed outside the battery outer case; and
a current shut-off mechanism placed on a conductive path from the collector terminal to the outwardly exposed terminal and configured to cut off the conductive path when an internal pressure of the battery outer case exceeds a predetermined pressure; and
the current shut-off mechanism includes the connection plate as a plate-shaped conductive member provided in one end of the collector terminal, the connection plate with the vent hole provided in a central part of the connection plate, and the shut-off valve including the reversing portion electrically connected to the outwardly exposed terminal.

### Claim 11 (depends on 10)

The manufacturing method according to claim 10, wherein the reversing portion includes a dome-shaped concave portion that is concaved toward the inner side of the battery outer case.

### Claim 12 (depends on 10)

The manufacturing method according to claim 10, wherein, when the metallic material is sprayed to the border between the joint region and the reversing portion, any one of plasma spraying, flame spraying, electric arc spraying, and cold spray is used.

### Claim 13 (depends on 10)

The manufacturing method according to claim 10, wherein, when the metallic material is sprayed, a distance from a tip end of a thermal-spray nozzle that sprays the metallic material to the border is from 250 mm to 350 mm.

### Claim 14 (depends on 10)

The manufacturing method according to claim 10, wherein, when the metallic material is sprayed, the thermal-spray joint portion is formed at 200° C. or less.