Method for manufacturing pneumatic tire
AssigneeThe Yokohama Rubber Co., Ltd.
InventorsShun Sato, Hideki Seto
Life of this patent
Estimating the term…
Abstract
A method for manufacturing a pneumatic tire may include lap-splicing end parts of a laminate sheet in which a sheet obtained from a thermoplastic resin or a thermoplastic resin composition of a thermoplastic resin blended with an elastomer is laminated with a rubber that undergoes vulcanizing adhesion with the thermoplastic resin or the thermoplastic resin composition. After the sheet obtained from the thermoplastic resin or the thermoplastic resin composition is cut into lengths to be supplied for lap-splicing, and at a stage before tire vulcanization molding, distal end parts of the sheet obtained from the thermoplastic resin or the thermoplastic resin composition are sharpened with a thermal treatment.
Claims11
A method for manufacturing a pneumatic tire, comprising:
- lap splicing end parts of a laminate sheet comprising a thermoplastic sheet obtained from a thermoplastic resin or a thermoplastic resin composition, the composition comprising a thermoplastic resin blended with an elastomer, and the thermoplastic sheet being laminated with a rubber that undergoes vulcanizing adhesion with the thermoplastic resin or the thermoplastic resin composition;
- and
- sharpening distal end parts of the thermoplastic sheet obtained from the thermoplastic resin or the thermoplastic resin composition with a thermal treatment after the thermoplastic sheet obtained from the thermoplastic resin or the thermoplastic resin composition is cut into lengths to be supplied to the lap-splicing step, and at a stage before tire vulcanization molding, before the lap-splicing, and before lamination of the thermoplastic sheet with the rubber, wherein the sharpening has a relationship in which a thickness T (mm) at a position at a distance inward by a length of (t×⅓) from the distal end of the thermoplastic sheet obtained from the thermoplastic resin or the thermoplastic resin composition satisfies the equation 0.1t≤T ≤0.8t, where
- t:
- average thickness (mm) in the tire circumferential direction of a portion not subject to the sharpening of the thermoplastic sheet obtained from the thermoplastic resin or the thermoplastic resin composition of a thermoplastic resin blended with an elastomer, and
- T:
- thickness (mm) at a position at a distance inward by a length of (t×⅓) from the distal end of the thermoplastic sheet obtained from the thermoplastic resin or the thermoplastic resin composition of a thermoplastic resin blended with an elastomer.