Manufacture method for a projection capacitive touch screen
AssigneeSuzhou Touch Planet Co., Ltd.
InventorYanting Luo
Life of this patent
Estimating the term…
Abstract
A manufacture method for a projection capacitive touch screen, includes following steps: (1) placing a clean PET substrate on a 3D printing platform, (2) the 3D printing platform outputting movement of x, y and z directions through control software, (3) aligning tail-throwing leads on the PET-X film, (4) tearing off the protective release film on one side of the PET-Y film, (5) bonding the PET-Y film and the PET-X film, (6) cutting off the redundant areas around the PET-XY film completed in the step (5), (7) drying the PET-XY film, and (8) laser welding the dried PET-XY film to obtain a projection capacitive touch screen.
Claims10
A manufacture method for a projection capacitive touch screen, comprising the following steps:
- (1) placing a clean PET substrate on a 3D printing platform, wherein said PET substrate is scratch-resistant with a release film to protect single-sided adhesive layer and its scratch-resistant surface is placed facing down, the PET substrate being fixed to the surface of the 3D printing platform by means of an adsorption device for the 3D printing platform, then tearing off the top release film to expose the adhesive layer in order to form a PET-X film;
- (2) moving in the three directions of X, Y and Z on the 3D printing platform by the control software, wherein the movement in the Z direction ensures the distance between the outlet of a wire barrel and the PET-X film of the substrate to be maintained at 0 to 0.5 mm, in the moving process of X, Y directions, enameled wires being adsorbed on the PET-X film and forming the designed graphics;
- (3) printing row lines on the PET-X film, aligning tail-throwing leads on the PET-X film, the conductive surface of the flexible tail-throwing circuit board with the tinned fingers being downwards attached to the row lines of the PET-X film, and then uniformly spraying the detergent solution on the surface of the PET-X film;
- (4) tearing off the protective release film on one side of the PET-Y film, which is a double-sided adhesive layer with a release film for protection, placing it on the platform with the exposed side of adhesive layer facing up, then evenly spraying detergent solution;
- (5) bonding the surface of the exposed adhesive layer of the PET-Y film sprayed with the detergent solution to the surface of the PET-X film exposed adhesive layer, and uniformly scraping the detergent solution between the PET-X film and the PET-Y film by a scraper or a scraping plate, so that no detergent solution residue is remained between the PET-X film and the PET-Y film, and a PET-XY film is formed;
- (6) cutting off the redundant areas around the PET-XY film completed in the step (5);
- (7) drying the PET-XY film completed in step (6) in a ventilation drying device;
- and
- (8) laser welding the PET-XY film which is completely dried in the step (7), melting the paint of the enameled wire thoroughly, then welding enameled wire and the tinned fingers of the flexible circuit board to obtain a projection capacitive touch screen.
Dependencies are inferred from the claim text.