# US 10,370,527 B2 · Polyethylene compositions having living hinge properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,370,527 B2
- Document ID: US10370527B2
- Status: Granted
- Kind: B2
- Application number: 15/534,383
- Filed: 2015-11-05
- Published: 2017-11-30
- Granted: 2019-08-06
- Earliest claimed: 2014-12-11
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Stephanie M. Whited; Mridula Babli Kapur; Yijian Lin
- Web page: https://patentgrep.com/patent/US10370527B2

## CPC

- C08L 23/06: Polyethylene
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2207/062: HDPE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A polyethylene composition suitable for use in a living hinge component, the composition comprising a first ethylene-based polymer component, the first ethylene-based polymer component has a density of from 0.91.5 g/cc to less than 0.940 g/cc. and a melt index, I2.16, of less than 5 g/10 min. and a second ethylene-based polymer component, wherein the composition has an overall density of from 0.945 g/cc to 0.960 g/cc and an overall melt index, I2.16, of from 5 g/10 min to 20 g/10 min.

## Claims

### Claim 1

A polyethylene composition suitable for use in a living hinge component, the composition comprising:
a first ethylene-based polymer component, the first ethylene-based polymer component has a density of from 0.915 g/cc to less than 0.940 g/cc, a melt index, I2.16, of less than 5 g/10 min, and an overall melt flow ratio (I21.6/I2.16) of 15 to 34; and
a second ethylene-based polymer component;
wherein the composition has an overall density of from 0.945 g/cc to 0.960 g/cc and an overall melt index, I2.16, of from 5 g/10 min to 20 g/10 min.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the composition comprises from 5 wt. % to 70 wt. % of the first ethylene-based polymer component, and from 30 wt. % to about 95 wt. % of the second ethylene-based polymer component.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the composition has a melt flow ratio, I21.6/I2.16, of greater than 35.0.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the second ethylene-based polymer component has a density of 0.955 g/cc to 0.980 g/cc, wherein the density is determined according to the equation:
1
Overall
⁢
⁢
Composition
⁢
⁢
Density
=
Wt
.
⁢
%
⁢
⁢
of
⁢
⁢
1
⁢
st
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
⁢
Density
⁢
⁢
of
⁢
⁢
1
⁢
st
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
+
Wt
.
⁢
%
⁢
⁢
of
⁢
⁢
2
⁢
nd
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
Density
⁢
⁢
of
⁢
⁢
2
⁢
nd
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the composition has a molecular weight distribution of 4.0 to 10.0.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the composition is prepared by in-situ interpolymerization using at least two reactors.

### Claim 7 (depends on 6)

The composition of claim 6, wherein the at least two reactors are operated in series.

### Claim 8

A living hinge component comprising a polyethylene composition, the composition comprising:
a first ethylene-based polymer component, the first ethylene-based polymer component has a density of from 0.915 g/cc to less than 0.940 g/cc, a melt index, I2.16, of less than 5 g/10 min, and an overall melt flow ratio (I21.6/I2.16) of 15 to 34; and
a second ethylene-based polymer component;
wherein the composition has an overall density of from 0.945 g/cc to 0.960 g/cc and an overall melt index, I2.16, of from 5 g/10 min to 20 g/10 min.

### Claim 9 (depends on 8)

The component of claim 8, wherein the composition comprises from 5 wt. % to 70 wt. % of the first ethylene-based polymer component, and from 30 wt. % to about 95 wt. % of the second ethylene-based polymer component.

### Claim 10 (depends on 8)

The component of claim 8, wherein the composition has a melt flow ratio, I21.6/I2.16, of greater than 35.

### Claim 11 (depends on 8)

The component of claim 8, wherein the second ethylene-based polymer component has a density of 0.955 g/cc to 0.980 g/cc, wherein the density is determined according to the equation:
1
Overall
⁢
⁢
Composition
⁢
⁢
Density
=
Wt
.
⁢
%
⁢
⁢
of
⁢
⁢
1
⁢
st
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
⁢
Density
⁢
⁢
of
⁢
⁢
1
⁢
st
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
+
Wt
.
⁢
%
⁢
⁢
of
⁢
⁢
2
⁢
nd
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
Density
⁢
⁢
of
⁢
⁢
2
⁢
nd
⁢
⁢
ethylene
-
based
⁢
⁢
polymer
.

### Claim 12 (depends on 8)

The component of claim 8, wherein the composition has a molecular weight distribution of 4.0 to 10.0.