Abstract
Disclosed herein is a method for applying metals to clay. More particularly, the present invention relates to applying malleable metals, such as silver, to clay, such that the metal attaches to the clay and as an added feature forms beads on the surface of the clay.
Claims2
A method for applying metal to clay comprising the ordered steps of:
- a. forming a piece of clay into a desired shape;
- b. drying the piece for 24-96 hours;
- c. baking the piece in a kiln at 1560°-2100° F.;
- d. allowing the piece to cool to room temperature;
- e. applying a colored or clear slip having a matte finish to the piece;
- f. baking the piece in the kiln at 1560°-2100° F.;
- g. allowing the piece to cool to room temperature;
- h. applying a silver precious metal clay in liquid form to the piece using a brush;
- i. baking the piece in the kiln at 1940° F. so that the silver precious metal forms a plurality of beads of silver on a surface of the piece,
- wherein the plurality of beads are each visible to the naked eye and form an irregular pattern on the surface of the piece;
- and
- j. allowing the piece to cool to room temperature in the kiln.
9 more elements
A method for applying metal to clay consisting of the ordered steps of:
- a. forming a piece of clay into a desired shape;
- b. drying the piece for 24-96 hours;
- c. baking the piece in a kiln at 1830° F.;
- d. allowing the piece to cool to room temperature;
- e. applying a colored or clear slip having a matte finish to the piece;
- f. baking the piece in the kiln at 1830° F.;
- g. allowing the piece to cool to room temperature;
- h. applying a silver precious metal clay in liquid form to the piece using a brush;
- i. baking the piece in the kiln at 1940° F. so that the silver precious metal forms a plurality of beads of silver on a surface of the piece;
- wherein the plurality of beads are each visible to the naked eye and form an irregular pattern on the surface of the piece;
- and
- j. allowing the piece to cool to room temperature in the kiln.