# US 10,312,668 B2 · Spark plug having firing pad

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,312,668 B2
- Document ID: US10312668B2
- Status: Granted
- Kind: B2
- Application number: 15/585,907
- Filed: 2017-05-03
- Published: 2017-08-17
- Granted: 2019-06-04
- Earliest claimed: 2012-08-09
- Assignees: Federal-Mogul Ignition Company
- Applicants: Federal-Mogul Ignition Company
- Inventors: Kevin J. Kowalski; Frederick J. Quitmeyer; Nathan A. Thomson; Curtis W. Verhoff; Richard L. Keller
- Web page: https://patentgrep.com/patent/US10312668B2

## CPC

- H01T 13/20: characterised by features of the electrodes or insulation
- H01T 13/39: Selection of materials for electrodes
- H01T 21/02: of sparking plugs
- H01T: SPARK GAPS; OVERVOLTAGE ARRESTERS USING SPARK GAPS; SPARKING PLUGS; CORONA DEVICES; GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES (overvoltage protection circuits H02H)

## Abstract

A spark plug has a firing pad attached to a center electrode or to a ground electrode. The firing pad is attached via laser welding and has a sparking surface with an overall fused area and an unfused area. In one or more embodiments, the overall fused area is located in part or more inboard of a peripheral edge of the firing pad.

## Claims

### Claim 1

A method of attaching a firing pad to an electrode for a spark plug, comprising the steps of:
initially applying a laser beam at a weld starting point located outboard of a peripheral edge of the firing pad and forming one or more fused portion(s), wherein at least one of the one or more fused portion(s) is formed on the electrode;
moving the laser beam from the weld starting point so that the laser beam crosses the peripheral edge of the firing pad;
applying the laser beam to the sparking surface of the firing pad to produce a fused area subject to application of the laser beam and an unfused area not subject to application of the laser beam;
maintaining the laser beam at the sparking surface of the firing pad so that a weld is formed between the firing pad and the electrode, wherein at least one of the one or more fused portion(s) have an overall fused area that is located largely or entirely inboard of the peripheral edge of the firing pad to form at least one of the one or more fused portion(s) on the sparking surface of the firing pad; and
controlling the laser beam to leave at least one unfused portion at the sparking surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the applying step comprises applying the laser beam to the sparking surface for a first duration to produce a first discrete individual fused portion and for a second duration to produce a second discrete individual fused portion.

### Claim 3 (depends on 2)

The method of claim 2, wherein the first discrete individual fused portion and the second discrete individual fused portion at least partially overlap.

### Claim 4 (depends on 1)

The method of claim 1, further comprising the steps of:
moving the laser beam from the sparking surface so that the laser beam again crosses the peripheral edge of the firing pad; and
stopping the laser beam at a weld stopping point located outboard of the peripheral edge and again forming at least one of the one or more fused portion(s) on the electrode, wherein at least a portion of the peripheral edge remains unfused.

### Claim 5

A method of attaching a firing pad to an electrode for a spark plug, comprising the steps of:
initially applying a laser beam at a weld starting point located inboard of a peripheral edge of the firing pad and forming one or more fused portion(s) on a sparking surface, wherein the laser beam is applied to the sparking surface of the firing pad to produce a fused area subject to application of the laser beam and an unfused area not subject to application of the laser beam;
maintaining the laser beam at the sparking surface of the firing pad so that a weld is formed between the firing pad and the electrode, wherein the laser beam creates one or more fused portion(s) that have an overall fused area that is located largely or entirely inboard of a peripheral edge of the firing pad;
controlling the laser beam to leave at least one unfused portion at the sparking surface;
moving the laser beam from the weld starting point so that the laser beam crosses the peripheral edge of the firing pad; and
forming at least one of the one or more fused portion(s) on the electrode.

### Claim 6 (depends on 5)

The method of claim 5, further comprising the steps of:
moving the laser beam from the weld starting point so that the laser beam again crosses the peripheral edge of the firing pad; and
stopping the laser beam at a weld stopping point located outboard of the peripheral edge and again forming at least one of the one or more fused portion(s) on the electrode, wherein at least a portion of the peripheral edge remains unfused.

### Claim 7

A method of attaching a firing pad to an electrode for a spark plug, comprising the steps of:
initially applying a laser beam to a sparking surface of the firing pad or the electrode outboard of a peripheral edge of the firing pad;
moving the laser beam from the sparking surface of the firing pad to the electrode outboard of the peripheral edge of the firing pad or causing the laser beam to move from the electrode outboard of the peripheral edge of the firing pad to the sparking surface of the firing pad, wherein the laser beam crosses the peripheral edge of the firing pad as the laser beam moves;
forming one or more fused portion(s) on the electrode while the laser beam moves; and
forming one or more fused portion(s) on the sparking surface of the firing pad while the laser beam moves.

### Claim 8 (depends on 7)

The method of claim 7, wherein the initially applying step applies the laser beam to the electrode outboard of the peripheral edge of the firing pad.

### Claim 9 (depends on 8)

The method of claim 8, further comprising the step of:
moving the laser beam to the electrode outboard of the peripheral edge of the firing pad after movement of the laser beam from the electrode outboard of the peripheral edge to the sparking surface so that a weld starting point is located on the electrode outboard of the peripheral edge of the firing pad and a weld stopping point is located on the electrode outboard of the peripheral edge of the firing pad.

### Claim 10 (depends on 9)

The method of claim 9, wherein at least a portion of the peripheral edge remains unfused.

### Claim 11 (depends on 7)

The method of claim 7, wherein the initially applying step applies the laser beam to the sparking surface inboard of the peripheral edge of the firing pad.

### Claim 12 (depends on 11)

The method of claim 11, further comprising the step of:
moving the laser beam to the sparking surface after movement of the laser beam from the sparking surface to the electrode outboard of the peripheral edge of the firing pad so that a weld starting point is located on the sparking surface and a weld stopping point is located on the sparking surface.

### Claim 13

A method of attaching a firing pad to an electrode for a spark plug, comprising the steps of:
striking a sparking surface of the firing pad with a laser beam;
penetrating entirely through a thickness of the firing pad with the laser beam;
mixing a material of the firing pad with a material of the electrode to form one or more fused portion(s) as thermal energy from the laser beam increases at a surface-to-surface interface between the firing pad and the electrode, wherein an unfused portion exists between the fused portion and a peripheral edge of the firing pad;
moving the laser beam from the sparking surface across the peripheral edge of the firing pad;
forming at least one of the one or more fused portion(s) on the electrode while the laser beam moves; and
forming at least one of the one or more fused portion(s) on the sparking surface of the firing pad while the laser beam moves.

### Claim 14 (depends on 13)

The method of claim 13, wherein the mixed material of the firing pad and the electrode has a different rate of thermal expansion than the unfused portion of the sparking surface.

### Claim 15 (depends on 13)

The method of claim 13, wherein the mixing step includes forming a greater ratio of firing pad material to electrode material near the sparking surface.

### Claim 16 (depends on 13)

The method of claim 13, wherein a width of the firing pad is at least twice as large as the thickness of the firing pad.

### Claim 17 (depends on 13)

The method of claim 13, further comprising the step of resistance welding the firing pad to the electrode before the striking step.

### Claim 18 (depends on 17)

The method of claim 17, wherein the firing pad includes a plurality of protrusions that project from a bottom surface of the firing pad toward the surface-to-surface interface between the firing pad and the electrode.