# US 10,245,804 B2 · Fire retarded aramid fiber-based honeycomb

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,245,804 B2
- Document ID: US10245804B2
- Status: Granted
- Kind: B2
- Application number: 14/885,896
- Filed: 2015-10-16
- Published: 2017-04-20
- Granted: 2019-04-02
- Earliest claimed: 2015-10-16
- Assignees: Hexcel Corporation
- Applicants: Hexcel Corporation
- Inventors: Lance Smith; Yen-Seine Wang
- Web page: https://patentgrep.com/patent/US10245804B2

## CPC

- B32B 3/12: characterised by a layer of regularly- arranged cells, e.g. a honeycomb structure
- B32B 5/20: foamed in situ
- D21H 5/0002: {Flame-resistant papers; (complex) compositions rendering paper fire-resistant}
- D21H 13/26: Polyamides; Polyimides
- D21H 19/24: comprising macromolecular compounds obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds
- D21H 23/22: Addition to the formed paper
- B32B 2250/02: 2 layers
- B32B 2255/02: on fibrous or filamentary layer
- B32B 2255/26: Polymeric coating
- B32B 2262/0269: Aromatic polyamide fibres
- B32B 2307/3065: Flame resistant or retardant, fire resistant or retardant
- B32B 2605/18: Aircraft
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

An alternate resin-coated paper material for use in making honeycomb. The alternate resin-coated paper material is made from a paper that contains from 30 to 50 weight percent aramid fibers and from 50 to 70 weight percent of non-aramid fibers. A fire retarded phenolic resin is incorporated into the paper to make it self-extinguishing in less than 10 seconds with a self-extinguishing burn length of less than 12 inches when exposed to a 12-second vertical flame in accordance with the vertical burn test requirements set forth in 14 C.F.R. Part 25.583. The fire retarded phenolic resin includes a phenol formaldehyde resin and a phosphorous-containing fire retardant.

## Claims

### Claim 1

A honeycomb for use in making aircraft panels wherein said honeycomb has walls comprising a resin-coated paper material that has a self-extinguishing time of less than 10 seconds and a self-extinguishing burn length of less than 12 inches when exposed to a 12 second vertical flame in accordance with the vertical burn test requirements set forth in 14 C.F.R. Part 25.583, said resin-coated paper material comprising:
a. layer of paper comprising from 30 to 50 weight percent para-aramid fibers and para-aramid pulp, based on the total weight of said paper, and from 50 to 70 weight percent non-aramid fibers and non-aramid pulp, based on the total weight of said paper, said non-aramid fibers being selected from the group consisting of polyester fibers and acrylic fibers and said non-aramid pulp comprising, cellulose fibers; and
a fire retarded phenolic resin comprising a phenol formaldehyde resin and a sufficient amount of a phosphorous-containing fire retardant so that said fire retarded phenolic resin contains from 2 to 6 weight percent phosphorous, wherein the amount of said fire retarded phenolic resin in said resin-coated paper material is sufficient to so that said resin-coated paper material has a self-extinguishing time of less than 10 seconds and a self-extinguishing burn length of less than 12 inches when exposed to a 12-second vertical flame in accordance with the vertical burn test requirements set forth in 14 C.F.R. Part 25.583.

### Claim 2 (depends on 1)

The honeycomb for use in making aircraft panels according to claim 1 wherein said resin-coated paper material comprises from 40 to 65 weight percent of said fire retarded phenolic resin, based on the total weight of said honeycomb walls.

### Claim 3 (depends on 1)

The honeycomb for use in making aircraft panels according to claim 1 wherein said phosphorous-containing fire retardant is a phenoxyphosphazene.

### Claim 4 (depends on 1)

The honeycomb for use in making aircraft panels according to claim 1 wherein said phosphorous-containing fire retardant is a phosphonate oligomer.

### Claim 5 (depends on 1)

A panel that comprises the honeycomb, according to claim 1 and a face sheet that is bonded to said honeycomb.

### Claim 6 (depends on 1)

The honeycomb for use in making aircraft panels according to claim 1 wherein the amount of para-aramid pulp in said paper is from 15 to 35 weight percent, based on the total weight of the para-aramid fibers and para-aramid pulp.

### Claim 7 (depends on 6)

The honeycomb for use in making aircraft panels according to claim 6 wherein the amount of non-aramid pulp in said paper is from 15 to 35 weight percent, based on the total weight of the non-aramid fibers and non-aramid pulp.

### Claim 8 (depends on 1)

The honeycomb for use in making aircraft panels according to claim 1 wherein the amount of non-aramid pulp in said paper is from 15 to 35 weight percent, based on the total weight of the non-aramid fibers and non-aramid pulp.