Thermal energy storage and heat insulation polyester fiber, and preparation method therefor
AssigneeHyosung Tnc Corporation
InventorsSung Jin Oh, Min Suk Lee
Life of this patent
Estimating the term…
Loading patent…
AssigneeHyosung Tnc Corporation
InventorsSung Jin Oh, Min Suk Lee
Estimating the term…
The present invention is directed to a method for preparing a polyester fiber, the method including: mixing 5-50 wt % of composite metal oxide particles, including a tungsten-based oxide, a cesium-based oxide, an antimony-based oxide, an indium-based oxide, and a tin-based oxide, with 40-90 wt % of one or two types of organic solvents selected from among alcohol, ketone, and acetates, 0.4-20 wt % of polyvinyl butyral, i.e., polymer, and 2-30 wt % of calcium stearate or magnesium stearate to obtain a mixture, and stirring and grinding the mixture to prepare a dispersion liquid; drying the dispersion liquid to prepare a powdered additive; mixing 1-30 wt % of the additive with polyester chips to obtain a mixture and melting this mixture to prepare master batch chips; and mixing 1-10 wt % of the master batch chips with general polyester chips to obtain a mixture, and melting and spinning this mixture.
A polyester fiber comprising 0.01-2 wt % of composite metal oxide particles in which a tungsten-based oxide, a cesium-based oxide, an antimony-based oxide, an indium-based oxide, and a tin-based oxide are mixed.
A method for preparing a polyester fiber, the method comprising:
Dependencies are inferred from the claim text.