Fcc materials of aluminum, cobalt, iron and nickel, and products made therefrom
AssigneeArconic Inc.
InventorsJen Lin, Xinyan Yan
Life of this patent
Estimating the term…
Abstract
The present disclosure relates to new materials comprising Al, Co, Fe, and Ni. The new materials may realize a single phase field of a face-centered cubic (fcc) solid solution structure immediately below the solidus temperature of the material. The new materials may include at least one precipitate phase and have a solvus temperature of at least 1000° C. The new materials may include 4.4-11.4 wt. % Al, 4.9-42.2 wt. % Co, 4.6-28.9 wt. % Fe, and 44.1-86.1 wt. % Ni. In one embodiment, the precipitate is selected from the group consisting of the L12 phase, the B2 phase, and combinations thereof. The new alloys may realize improved high temperature properties.
Claims19
A composition of matter comprising:
- 4.4-11.4 wt. % Al;
- 4.9-42.2 wt. % Co;
- 4.6-28.9 wt. % Fe;
- and
- 57.4-86.1 wt. % Ni;
- the balance being any optional incidental elements and impurities.
An alloy body comprising:
- 4.4-11.4 wt. % Al;
- 4.9-42.2 wt. % Co;
- 4.6-28.9 wt. % Fe;
- and
- 57.4-86.1 wt. % Ni;
- the balance being any optional incidental elements and impurities.