# US 10,144,670 B2 · Chemically strengthened glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,144,670 B2
- Document ID: US10144670B2
- Status: Granted
- Kind: B2
- Application number: 15/804,511
- Filed: 2017-11-06
- Published: 2018-03-08
- Granted: 2018-12-04
- Earliest claimed: 2015-05-15
- Assignees: AGC Inc.
- Applicants: Asahi Glass Company, Limited
- Inventors: Kosho Akatsuka; Satoshi Ogami
- Web page: https://patentgrep.com/patent/US10144670B2

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/085: containing an oxide of a divalent metal
- C03C 4/18: for ion-sensitive glass
- C03C 2201/00: Glass compositions
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention relates to a chemically strengthened glass, in which CT1 and CT5 satisfy CT5/CT1≤0.85, the CT1 satisfies CT1>−38.7×ln(t/1000)+48.2 [MPa] and an internal energy density rE satisfies rE≤23.3×t/1000+15 [kJ/m2]. CS is a surface compressive stress value [MPa], σ (x) is a compressive stress value [MPa] at a position x in a depth direction, DOL is a compressive stress depth [μm], and t is a sheet thickness [μm].

## Claims

### Claim 1

A chemically strengthened glass, wherein:
a CT1 obtained by formula (1) and an internal tensile stress CT5 obtained by formula (5) satisfy CT5/CT1≤0.85;
the internal tensile stress CT5 is 30 MPa or more;
a compressive stress value at a depth of a half value of the compressive stress depth DOL from the surface of the chemically strengthened glass is 10% or less of the surface compressive stress CS;
when a sheet thickness of the chemically strengthened glass is t (μm), the CT1 satisfies CT1>−38.7×ln(t/1000)+48.2 [MPa]; and
an internal energy density rE obtained by formula (6) satisfies rE≤23.3×t/1000+15 [kJ/m2]:
CT
1
=
CS
×
DOL
(
t
-
2
×
DOL
)
(
1
)
CT
5
=
2
×
∫
0
DOL
⁢
σ
⁡
(
x
)
⁢
dx
(
t
-
2
×
DOL
)
(
5
)
rE
=
CT
5
×
(
t
-
2
×
DOL
)
2
1000
×
t
(
6
)
wherein
CS is a surface compressive stress value [MPa] of the chemically strengthened glass,
σ (x) is a compressive stress value [MPa] at a position x in a depth direction from a surface of the chemically strengthened glass,
DOL is a compressive stress depth [μm] of the chemically strengthened glass, and
t is a sheet thickness [μm] of the chemically strengthened glass.

### Claim 2 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the surface compressive stress CS is 600 MPa or more.

### Claim 3 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the compressive stress depth DOL is 30 μm or more.

### Claim 4 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the sheet thickness t is 1500 μm or less.

### Claim 5 (depends on 1)

The chemically strengthened glass according to claim 1, wherein a position HW having a compressive stress being a half value of the surface compressive stress CS is a position less than 8 μm from the surface of the chemically strengthened glass.

### Claim 6 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 satisfies CT5>−38.7×ln(t/1000)+48.2 [MPa].

### Claim 7 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 1.1 times or more a CTlimit value [MPa] obtained by formula (2):
CTlimit=−38.7×ln(t/1000)+48.2 (2),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 8 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 1.1 times or more a CTlimit value [MPa] obtained by formula (4):
CTlimit=−36.7×ln(t/1000)+48.7 (4),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 9 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the CT1 [MPa] is 1.1 times or more a CTlimit value [MPa] obtained by formula (2):
CTlimit=−38.7×ln(t/1000)+48.2 (2),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 10 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the CT1 [MPa] is 1.1 times or more a CTlimit value [MPa] obtained by formula (4):
CTlimit=−36.7×ln(t/1000)+48.7 (4),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 11 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 1.5 times or more a CTlimit value [MPa] obtained by formula (2):
CTlimit=−38.7×ln(t/1000)+48.2 (2),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 12 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 2.0 times or more a CTlimit value [MPa] obtained by formula (2):
CTlimit=−38.7×ln(t/1000)+48.2 (2),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 13 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 3.0 times or more a CTlimit value [MPa] obtained by formula (2):
CTlimit=−38.7×ln(t/1000)+48.2 (2),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 14 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 1.5 times or more a CTlimit value [MPa] obtained by formula (4):
CTlimit=−36.7×ln(t/1000)+48.7 (4),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 15 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 2.0 times or more a CTlimit value [MPa] obtained by formula (4):
CTlimit=−36.7×ln(t/1000)+48.7 (4),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.

### Claim 16 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the internal tensile stress CT5 [MPa] is 3.0 times or more a CTlimit value [MPa] obtained by formula (4):
CTlimit=−36.7×ln(t/1000)+48.7 (4),
wherein t is the sheet thickness [μm] of the chemically strengthened glass.