Active material, nonaqueous electrolyte battery, battery pack, and method of producing active material
AssigneeKabushiki Kaisha Toshiba
InventorsKazuki Ise, Yorikazu Yoshida, Yasuhiro Harada, Hiroki Inagaki, Norio Takami
Life of this patent
Estimating the term…
Abstract
According to one embodiment, an active material containing a niobium titanium composite oxide is provided. The niobium titanium composite oxide has average composition represented by LiyNb2+xTi1−xO7+0.5x (0≤x≤0.5, 0≤y≤5.5). The niobium titanium composite oxide satisfies peak intensity ratios represented by the following formulae (1) to (3): 0.05≤(B/A)≤0.7 (1) 0.01≤(C/A)≤0.2 (2) 0≤(D/A)≤0.1 (3).
Claims20
An active material comprising a niobium titanium composite oxide whose average composition is represented by LiyNb2+xTi1−xO7+0.5x (0≤x≤0.5, 0≤y≤5.5) and which satisfies peak intensity ratios represented by the following formulae (1) to (3):
- 0.05≤(B/A)≤0.7 (1)
- 0.01≤(C/A)≤0.2 (2)
- 0≤(D/A)≤0.1 (3)
- wherein A is an intensity of a peak derived from Nb2TiO7 at 2θ of 26.0±0.1° in a wide angle X-ray diffraction pattern using CuKα rays as an X-ray source, B is an intensity of a peak derived from Nb10Ti2O29 at 2θ of 25.0±0.1° in the wide angle X-ray diffraction pattern, C is an intensity of a peak derived from Nb24TiO62 at 2θ of 24.8±0.1° in the wide angle X-ray diffraction pattern, and D is an intensity of a peak derived from a TiO2 rutile phase at 2θ of 27.4±0.2° in the wide angle X-ray diffraction pattern.