# US 10,081,574 B2 · Process for converting calcium bentonite to sodium bentonite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,081,574 B2
- Document ID: US10081574B2
- Status: Granted
- Kind: B2
- Application number: 15/587,852
- Filed: 2017-05-05
- Published: 2017-09-14
- Granted: 2018-09-25
- Earliest claimed: 2015-11-30
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Musaab Ibrahim Magzoub; Mustafa Saleh Nasser; Ibnelwaleed Ali Hussein; Mohamed Ahmed Nasr Eldin Mahmoud; Abdullah Saad Sultan
- Web page: https://patentgrep.com/patent/US10081574B2

## CPC

- C04B 33/04: Clay; Kaolin
- B28C 1/04: Producing suspensions, e.g. by blunging {or mixing; with means for removing stones}
- C01B 33/40: Clays
- C09K 8/032: {Inorganic additives}
- C04B 2235/349: Clays, e.g. bentonites, smectites such as montmorillonite, vermiculites or kaolines, e.g. illite, talc or sepiolite
- C09K 2208/34: Lubricant additives
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B28C: PREPARING CLAY; PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL, e.g. PLASTER (preparing material for foundry moulds B22C5/00)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Method of converting calcium bentonite to sodium bentonite that is suitable for use as drilling mud or a cement additive. After the addition of a calcium bentonite sample to a prepared soda ash solution at predetermined soda ash/bentonite weight ratios, the bentonite suspension is continuously heated and stirred for up to 24 h. The heating and stirring are crucial towards enhancing the sodium activation of the bentonite, as well as other rheological properties of the bentonite.

## Claims

### Claim 1

A method of converting calcium bentonite to sodium bentonite, comprising:
mixing a calcium bentonite sample with a sodium carbonate aqueous solution to form a bentonite suspension comprising calcium bentonite, sodium carbonate, and water,
wherein the sodium carbonate aqueous solution comprises no more than 1% by weight of sodium carbonate based on the total weight of the water in the sodium carbonate aqueous solution,
wherein the ratio of the weight of the sodium carbonate present in the sodium carbonate aqueous solution to the total weight of the calcium bentonite sample mixed with the sodium carbonate aqueous solution is 1:7 to 1:23, and
wherein after the mixing, a calcium bentonite concentration in the bentonite suspension is from 5 to 10 wt % based on a total weight of the water in the bentonite suspension; and
heating and stirring the bentonite suspension at below 80° C. for 6-24 hours to form a sodium bentonite product comprising water, sodium bentonite and calcium carbonate,
wherein the sodium bentonite product formed by the heating and stirring has a Na/Ca molar ratio of at least 2.5.

### Claim 2 (depends on 1)

The method of claim 1, wherein the sodium bentonite product formed by the heating and stirring has an apparent viscosity of at least 15 cP.

### Claim 3 (depends on 1)

The method of claim 1, wherein the sodium bentonite product formed by the heating and stirring has a yield point of no more than 30 lb/100 ft2.

### Claim 4 (depends on 1)

The method of claim 1, wherein the sodium bentonite product formed by the heating and stirring has a viscometer dial reading of 33-35 lb/100 ft2 at 300 rpm and 39-40 lb/100 ft2 at 600 rpm.

### Claim 5 (depends on 1)

The method of claim 1, wherein an average particle size of the sodium bentonite present in the sodium bentonite product is more than 500 times larger than an average particle size of the calcium bentonite sample added to the sodium carbonate aqueous solution.

### Claim 6 (depends on 1)

The method of claim 1, wherein the calcium bentonite sample is a raw bentonite sample.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
purifying the calcium bentonite sample by at least one method selected from the group consisting of dry-sieving, wet-sieving, dispersion in deionized water with hexametaphosphate, dispersion in deionized water without hexametaphosphate and sedimentation.

### Claim 8 (depends on 1)

The method of claim 1, wherein the sodium carbonate aqueous solution has a sodium carbonate concentration of 0.28-0.86% by weight based on a total weight of water.

### Claim 9 (depends on 1)

The method of claim 1, wherein the ratio of the weight of the sodium carbonate present in the sodium carbonate aqueous solution to the total weight of the calcium bentonite sample added to the sodium carbonate aqueous solution is 1:20 to 1:23.

### Claim 10 (depends on 1)

The method of claim 1, wherein the heating and stirring includes heating the bentonite suspension at 65-70° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein the heating and stirring includes stirring the bentonite suspension for 12-24 hours.

### Claim 12 (depends on 1)

The method of claim 1, wherein the sodium bentonite product formed by the heating and stirring has a Na/Ca molar ratio of 2.8-3.0.

### Claim 13

A method of converting calcium bentonite to sodium bentonite, comprising:
mixing a calcium bentonite sample with a sodium carbonate aqueous solution to form a bentonite suspension comprising calcium bentonite, sodium carbonate, and water,
wherein the sodium carbonate aqueous solution comprises no more than 1% by weight of sodium carbonate based on the total weight of the water in the sodium carbonate aqueous solution,
wherein the ratio of the weight of the sodium carbonate present in the sodium carbonate aqueous solution to the total weight of the calcium bentonite sample mixed with the sodium carbonate aqueous solution is 1:7 to 1:23, and
wherein after the mixing, a calcium bentonite concentration in the bentonite suspension is from 5 to 10 wt % based on a total weight of the water in the bentonite suspension; and
heating and stirring the bentonite suspension at below 80° C. for 6-24 hours to form a sodium bentonite product comprising water, sodium bentonite and calcium carbonate,
wherein the sodium bentonite present in the sodium bentonite product formed by the heating and stirring has a particle size of 1100-1400 μm.

### Claim 14 (depends on 1)

The method of claim 1, wherein the sodium bentonite product formed by the heating and stirring has a yield point of 12-28 lb/100 ft2.