# US 10,053,585 B2 · Flame-retardant polymer composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,053,585 B2
- Document ID: US10053585B2
- Status: Granted
- Kind: B2
- Application number: 14/419,189
- Filed: 2013-07-31
- Published: 2015-07-23
- Granted: 2018-08-21
- Earliest claimed: 2012-08-02
- Assignees: Bategu Gummitechnologie GmbH
- Applicants: Bategu Gummitechnologie GmbH & Co. KG
- Inventors: Gerhard Mestan
- Web page: https://patentgrep.com/patent/US10053585B2

## CPC

- C09D 7/61: inorganic
- C08L 7/00: Compositions of natural rubber
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L 9/02: Copolymers with acrylonitrile
- C08L 9/06: Copolymers with styrene
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C08L 23/32: by reaction with compounds containing phosphorus or sulfur
- C09D 5/18: Fireproof paints {including high temperature resistant paints}
- C09D 7/48: Stabilisers against degradation by oxygen, light or heat
- C09D 123/32: by reaction with compounds containing phosphorus or sulfur
- C08L 2201/02: Flame or fire retardant/resistant
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08L 2205/03: containing three or more polymers in a blend
- Y10T 428/24802: Discontinuous or differential coating, impregnation or bond [e.g., artwork, printing, retouched photograph, etc.]
- Y10T 428/269: including synthetic resin or polymer layer or component
- Y10T 428/31649: Ester, halide or nitrile of addition polymer
- Y10T 428/31837: Including polyene monomers
- Y10T 428/31924: Including polyene monomers
- Y10T 442/2631: Coating or impregnation provides heat or fire protection
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a flame-proofed polymeric composition suitable for coating workpieces, containing a vinyl acetate-containing thermoplastic polymer and an unsaturated elastomer containing double bonds as polymeric components, wherein the polymeric components are present in the form of a homogeneous polymeric mixture, and a mixture matrix vulcanized exclusively by a sulphur or sulphur-containing crosslinking system is formed, wherein the sulphur crosslinking system extends across the entire matrix and permeates the matrix completely, and—at least one flame retardant or a combination of flame retardants. The invention further relates to articles produced therefrom, and to composite elements coated with this composition and to a method for producing the same.

## Claims

### Claim 1

A flame-resistant polymer composition, comprising:
a thermoplastic polymer containing vinyl acetate;
an unsaturated elastomer containing double bonds; and
at least one flame retardant or a combination of flame retardants, said thermoplastic polymer and said unsaturated elastomer intermixed to form a homogenous mixture, said homogenous mixture vulcanised exclusively with sulphur or a sulphur-containing crosslinking agent so that a continuous system of sulphur crosslinks extends uninterruptedly through an entirety of the mixture.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer is non-crosslinked, and the unsaturated elastomer is at least partially crosslinked via the sulphur crosslinks, and wherein the mixture does not contain crosslinks except the sulphur crosslinks.

### Claim 3 (depends on 1)

The composition of claim 1, wherein chains of the thermoplastic polymer and sulphur-crosslinked chains of the elastomer spatially overlap one another.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the sulphur crosslinks include polysulphide and mono-and di-sulphide bonds, wherein a content of the polysulphide bonds is between 40 and 50%, and a content of the mono- and di-sulphide bonds is between 50 and 60%, relative to a total crosslink density of the mixture.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the mixture is substantially monophasic.

### Claim 6 (depends on 1)

The composition of claim 1, wherein in a vulcanised state the homogenous mixture has elastomeric properties at a range of 150-200° C.

### Claim 7 (depends on 1)

The composition of claim 1, wherein in a vulcanized state the homogenous mixture has no melting peak measured by dynamic differential calorimetry in a temperature range of up to 200° C.

### Claim 8 (depends on 1)

The composition of claim 1, wherein in a vulcanized state the homogenous mixture has a loss factor defined as a ratio of loss to storage modulus in dynamic shearing stress of tan δ<0.3 in a temperature range from room temperature up to 200° C.

### Claim 9 (depends on 1)

The composition of claim 1, further comprising at least one of additives and excipients, said composition being produced by
mixing the thermoplastic polymer and the unsaturated elastomer to form the homogeneous mixture,
adding the sulphur or the sulphur-containing crosslinking agent, the flame retardants, and the additives and/or excipients, whilst strictly avoiding any crosslinking and/or vulcanisation,
after adding the sulphur or the sulphur-containing crosslinking agent, moulding and vulcanizing the mixture, wherein the vulcanizing is performed in absence of shearing stress.

### Claim 10 (depends on 1)

The composition of claim 1, produced by static vulcanisation, in the absence of shearing stress or dynamic vulcanisation.

### Claim 11 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer and the unsaturated elastomer are free of halogen.

### Claim 12 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer is a homopolymer, copolymer, or terpolymer of vinyl acetate.

### Claim 13 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer has a melting point or a melting range beginning at less than 150° C.

### Claim 14 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer has a vinyl acetate content of 40-75 wt %.

### Claim 15 (depends on 1)

The composition of claim 1, wherein the unsaturated elastomer is a homopolymer, copolymer, or a terpolymer consisting of or containing diene monomer units.

### Claim 16 (depends on 1)

The composition of claim 1, wherein the unsaturated elastomer is a rubber with an unsaturated side group or an ethylene-propylene-diene rubber (EPDM) containing non-conjugated diene monomer units, selected from the group of 1,3-butadiene, 2-methyl-1,3-butadiene (isoprene), 2,3-dimethyl-1,3-butadiene, 1,3-pentadiene, 1,3-cyclopentadiene, dicyclopentadiene, 2-methyl-1,3-pentadiene, 1,3-hexadiene, 1,4-hexadiene, 1,4-cyclohexadiene, tetrahydroindene, methyl tetrahydroindene, ethylidene norbornene or 5-ethylidene-2-norbornene (ENB), 5-methylene-2-norbornene (MNB), 1,6 octadiene, 5-methyl-1,4-hexadiene, 3,7-dimethyl-1,6-octadiene, 5-isolpropylidene-2-norbornene, 5-vinyl-norbornene (VNB), wherein the ethylene-propylene-diene rubber (EPDM) is a terpolymer consisting of ethylene, propylene, and 5-ethylidene-2-norbornene (ENB) or dicyclopentadiene (DCPD).

### Claim 17 (depends on 1)

The composition of claim 1, wherein the unsaturated elastomer is a rubber with an unsaturated main chain, wherein the unsaturated elastomer is partially hydrated and has a degree of hydration of 94-97%, and, prior to crosslinking, has a residual double bond content of 3-6% in the main chain relative to the initial double bond content in the main chain.

### Claim 18 (depends on 1)

The composition of claim 1, wherein the sulphur that forms the sulphur crosslinks is contained in the composition in an amount of 0.3-2 phr (parts per hundred rubber) relative to a total amount of polymer components.

### Claim 19 (depends on 18)

The composition of claim 18, wherein the sulphur is contained in an amount of at least 0.5 phr relative to a total amount of the polymer components.

### Claim 20 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer is non-crosslinked and is present in an amount of 5-15 wt %, and the unsaturated elastomer is present in an amount of 20-40 wt %, relative in each case to the total weight of the composition.

### Claim 21 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer mixture is non-crosslinked ethylene vinyl acetate (EVA) and the sulphur-crosslinked ethylene-propylene-diene rubber (EPDM) at a ratio of 40-20 wt % EVA to 60-80 wt % EPDM.

### Claim 22 (depends on 1)

The composition of claim 1, further comprising at least one polyolefin selected from the group consisting of polyethylene and polypropylene.

### Claim 23 (depends on 1)

The composition of claim 1, wherein the flame retardant(s) is/are present in an amount of 50-80 wt %, relative to the overall composition.

### Claim 24 (depends on 1)

The composition of claim 1, further comprising at least one of magnesium hydroxide (MDH), aluminium hydroxide (ATH), and zinc borate.

### Claim 25 (depends on 1)

The composition of claim 1, wherein the polymer containing vinyl acetate is present in an amount of 5-15 wt %, the unsaturated elastomer is present in an amount of 20-40 wt %, the flame retardant or flame retardants is/are present in an amount of 50-80 wt %, the remainder being excipient and additives.

### Claim 26 (depends on 1)

The composition of claim 1, having a hardness of 50-75, Shore A, and/or an ultimate elongation of 200-600% and/or a tear resistance of >7 N/mm.

### Claim 27

A method for producing a flame-resistant composition, comprising the steps in the order of:
mixing a thermoplastic polymer containing vinyl acetate, an unsaturated elastomer, a crosslinking agent, a flame retardant, and additives and excipients into a homogeneous mixture whilst avoiding crosslinking and/or vulcanisation,
moulding the mixture, and
vulcanizing the mixture during or at the end of moulding, as a static, non-dynamic vulcanisation that avoids shearing exclusively with sulphur or a sulphur-containing crosslinking agent so that a continuous system of sulphur crosslinks extends uninterruptedly through an entirety of the mixture.

### Claim 28 (depends on 27)

The method of claim 27, wherein the mixing is carried out at a temperature of no more than 125° C.

### Claim 29 (depends on 27)

The method of claim 27, wherein the moulding is carried out at a temperature of no more than 130° C.

### Claim 30 (depends on 27)

The method claim 27, wherein the vulcanisation occurs at a temperature of no more than 200° C. and at a pressure of 100-200 bar.

### Claim 31

A flame-retardant article comprising a composition comprising a thermoplastic polymer containing vinyl acetate, an unsaturated elastomer containing double bonds, and at least one flame retardant or a combination of flame retardants, said thermoplastic polymer and said unsaturated elastomer intermixed to form a homogenous mixture, said homogenous mixture vulcanised exclusively with sulphur or a sulphur-containing crosslinking agent so that a continuous system of sulphur crosslinks extends uninterruptedly through an entirety of the mixture.

### Claim 32 (depends on 1)

An elastic flame-retardant composite element, suited for vibration damping and suspension, said elastic flame-retardant composite element having a base, with at least a portion of an outer surface of the base having a coating made of a composition as set forth in claim 1.

### Claim 33 (depends on 32)

The composite element of claim 32, wherein the base is made primarily of rubber.

### Claim 34 (depends on 32)

The composite element of claim 32, wherein the coating is fixedly and inseparately attached to the base and is applied to the base by one of manufacture, extrusion, pressing, spraying, and subsequent coextrusion.

### Claim 35 (depends on 32)

The composite element of claim 32, wherein the coating has a thickness of less than 10 mm.

### Claim 36 (depends on 32)

The composite element of claim 32, wherein the coating has a weight percentage of 1-20 wt % of the elastic composite element.

### Claim 37 (depends on 32)

The composite element of claim 32, wherein the base has a reinforcement selected from the group consisting of fibres, glass fibres, polymer fibres, CFK fibres, GFK fibres, and a fabric.

### Claim 38 (depends on 32)

An article, comprising the composite element of claim 32, wherein the article is a spring element, damping element, gasket, hose, mat, moulding, protective clothing, or elastomer profile.

### Claim 39 (depends on 2)

The flame-resistant polymer composition of claim 2, wherein the sulfur crosslinks include at least one of mono-, di-, and polysulphide bonds.

### Claim 40 (depends on 5)

The flame-resistant polymer composition of claim 5, wherein the polymer mixture is free of elastomer particles or rubber domains with a mean diameter of more than 0.5 microns.

### Claim 41 (depends on 9)

The flame-resistant polymer composition of claim 9, wherein the sulphur or sulphur containing crosslinking agent is added at a temperature of no more than 110° C.

### Claim 42 (depends on 11)

The flame-resistant polymer composition of claim 11, wherein the composition is free of halogen.

### Claim 43 (depends on 12)

The flame-resistant polymer composition of claim 12, wherein the polymer containing vinyl acetate is selected from the group consisting of polyvinyl acetate (PVAc) and ethylene vinyl acetate (EVA).

### Claim 44 (depends on 15)

The flame-resistant polymer composition of claim 15, wherein the unsaturated elastomer is a terpolymer consisting of ethylene, propylene, and diene.

### Claim 45 (depends on 44)

The flame-resistant polymer composition of claim 44, wherein the diene has a content of at least 2-12 wt % relative to the terpolymer.

### Claim 46 (depends on 24)

The flame-resistant polymer composition of claim 24, wherein the flame retardants are solid and powdery or crystalline.

### Claim 47 (depends on 4)

The composition of claim 4, wherein the content of the polysulphide bonds is 45%, and the content of the mono- and di-sulphide bonds is 55%, relative to the total crosslink density of the mixture.

### Claim 48 (depends on 1)

The composition of claim 1, wherein the thermoplastic polymer has a melting point or a melting range beginning at less than 100° C.

### Claim 49 (depends on 17)

The composition of claim 17, wherein the unsaturated elastomer is a partially hydrated acrylonitrile butadiene rubber (HNBR).

### Claim 50 (depends on 20)

The composition of claim 20, wherein the thermoplastic polymer is present in an amount of 7-12 wt %, and the unsaturated elastomer is present in an amount of 20-30 wt %, relative in each case to the total weight of the composition.

### Claim 51 (depends on 21)

The composition of claim 21, wherein the ratio is approximately 20-30 wt % EVA to 70-80 wt % EPDM.

### Claim 52 (depends on 22)

The composition of claim 22, wherein the polyethylene is LLDPE.

### Claim 53 (depends on 1)

The composition of claim 1, wherein the flame retardant(s) is/are present in an amount of 60-70 wt %, relative to the overall composition.

### Claim 54 (depends on 1)

The composition of claim 1, having a hardness of 55-65, Shore A, and/or an ultimate elongation of 350-600% and/or a tear resistance of >9 N/mm.

### Claim 55 (depends on 27)

The method of claim 27, wherein the mixing is carried out at a temperature of 50-110° C.

### Claim 56 (depends on 27)

The method of claim 27, wherein the moulding is carried out at a temperature of 70-100° C.

### Claim 57 (depends on 27)

The method claim 27, wherein the vulcanisation occurs at a temperature which is higher than a temperature during mixing or moulding.

### Claim 58 (depends on 30)

The method claim 30, wherein the vulcanisation occurs at a temperature of 130-170° C.

### Claim 59 (depends on 33)

The composite element of claim 33, wherein the rubber is selected from the group consisting of polybutadiene rubber, styrene butadiene rubber, acrylonitrile rubber, ethylene-propylene-diene rubber, sponge rubber, any mixture thereof, and natural rubber.

### Claim 60 (depends on 32)

The composite element of claim 32, wherein the coating has a thickness of 1-5 mm.

### Claim 61 (depends on 32)

The composite element of claim 32, wherein the coating has a weight percentage of 2-16 wt % of the elastic composite element.