Storage stabilized devulcanized tire rubber modified asphalt composition and the process for its preparation
OwnerChandrasekaran Ramayya Pillai, Hari Chandrainventors
Life of this patent
Estimating the term…
Loading patent…
OwnerChandrasekaran Ramayya Pillai, Hari Chandrainventors
Estimating the term…
This invention relates to a storage stabilized recycled and devulcanized tire rubber modified asphalt composition, which comprises: 65.0 to 90.0% by weight of a neat asphalt, 3.0-50.0% by weight of a recycled and devulcanized rubber from used tires and/or other scrap rubbers, 0.01-15.0% by weight of a compatibilizer/stabilizer derived from Natural or Synthetic Rubbers, which composition passes the “cigar tube” softening point test difference of less than 5° C. between the top and bottom layers; and, the process for the said asphalt composition comprises mixing 65.0% to 90.0% by weight of a neat asphalt, 3.0 to 50.0% by weight of a recycled and devulcanized rubber from used tires, 0.01-10.0% by weight of a compatibilizer/stabilizer derived from Natural or Synthetic Rubbers, using high shear mixers at elevated temperatures of between 120° C. and 175° C. for between 15 minutes to 6 hours, to obtain storage stabilized asphalt composition that is stable in hot storage and transportation conditions.
A process for making a storage stable devulcanized tire rubber modified asphalt binder comprising:
Dependencies are inferred from the claim text.